Method for producing components with a high load capacity from TiAl alloys
Abstract
The invention relates to a method for producing components with a high load capacity from α+γ TiAl alloys, especially for producing components for aircraft engines or stationary gas turbines. According to this method, enclosed TiAl blanks of globular structure are preformed by isothermal primary forming in the α+γ− or α phase area. The preforms are then shaped out into components with a predeterminable contour by means of at least one isothermal secondary forming process, with dynamic recrystallization in the α+γ− or α phase area. The microstructure is adjusted by solution annealing the components in the α phase area and then cooling them off rapidly.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 8.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for producing heavy-duty components from α+γ TiAl alloys for aircraft engines or stationary gas turbines, in that preshaping encapsulated TiAl preforms of globular structure by isothermal primary shaping in the α+γ or α phase area in a temperature region of 1000° C. to 1,340° C. by forging or extrusion molding; shaping the preforms by forging to form components with a specifiable contour by at least one isothermal secondary shaping process simultaneously with dynamic recrystallization in the α+γ or α phase area in the temperature region of 1000° C. to 1,340° C. in an inert atmosphere,
- Claim 2Depends on #1
The method as defined in claim 1 , wherein the isotherma