Abstract

A semiconductor wafer with a front surface and a back surface and an epitaxial layer of semiconducting material deposited on the front surface, wherein the surface of the epitaxial layer has a maximum density of 0.14 localized light scatterers per cm 2 with a cross section of greater than or equal to 0.12 μm, and the front surface of the semiconductor wafer, prior to the deposition of the epitaxial layer, has a surface roughness of 0.05 to 0.29 nm RMS, measured by AFM on a 1 μm×1 μm reference area. There is also a process for producing a semiconductor wafer with a front surface and a back surface and an epitaxial layer of semiconducting material deposited on the front surface. The process includes the following: (a) a stock removal polishing step as the only polishing step; (b) cleaning and drying of the semiconductor wafer; (c) pretreatment of the front surface of the semiconductor wafer at a temperature of from 950 to 1250 degrees Celsius in an epitaxy reactor; and (d) deposition of the epitaxial layer on the front surface of the pretreated semiconductor wafer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a semiconductor wafer with a front surface and a back surface and an epitaxial layer of semiconducting material deposited on the front surface, wherein the process comprises the following process steps: a) a stock removal polishing step as the only polishing step: b) cleaning and drying of the semiconductor wafer; c) pretreating of the front surface of the semiconductor wafer in a first step in a hydrogen atmosphere at a temperature of 950° C. to 1250° C. to remove oxide from the front surface of the wafer, and then, in a second step, with a mixture of hydrogen and HCl

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • English Derwent Abstract AN 1999-519699 [44] corresp. to DE 198 33 257.
  • English Derwent Abstract AN 2000-579981 [55] corresp. to DE 199 05 737.
  • H.M. Liaw, J.W. Rose, Epitaxial Silicon Technology, Academic Press Inc., Orlando, Florida, 1986, p. 71-73.