A deposition method includes forming a nucleation layer over a substrate, forming a layer of a first substance at least one monolayer thick chemisorbed on the nucleation layer, and forming a layer of a second substance at least one monolayer thick chemisorbed on the first substance. The chemisorption product of the first and second substance may include silicon and nitrogen. The nucleation layer may comprise silicon nitride. Further, a deposition method may include forming a first part of a nucleation layer on a first surface of a substrate and forming a second part of a nucleation layer on a second surface of the substrate. A deposition layer may be formed on the first and second parts of the nucleation layer substantially non-selectively on the first part of the nucleation layer compared to the second part. The first surface may be a surface of a borophosphosilicate glass layer. The second surface may be a surface of a rugged polysilicon layer. The first and second part of the nucleation layer may be formed simultaneously.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A low selectivity deposition method comprising: forming a nucleation layer comprising silicon and nitrogen substantially non-selectively on a first and a second surface of a substrate by non-selective chemical vapor deposition; forming a monolayer of a first substance chemisorbed on the nucleation layer; and forming a monolayer of a second substance chemisorbed on the first substance, wherein a chemisorption product of the first and second substances comprises silicon nitride.

  2. Claim 2Depends on #1

    The deposition method of claim 1 wherein the nucleation layer comprises silicon nitride and a nucleation layer part that is over the first surface further comprises oxygen.

  3. Claim 3Depends on #1

    The deposition method of claim 1 wherein a thickness of the nucleation layer comprises less than about 20 Angstroms.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,785,853 AContinuous deposition reactor197468
US 4,058,430 AMethod for producing compound thin films19771,251
US 4,369,105 ASubstituted cobalt oxide spinels198326
US 4,831,003 ACatalyst composition and process of making198957
US 4,913,090 AChemical vapor deposition apparatus having cooling heads adjacent to gas dispersing heads in a single chamber199077
US 5,124,278 AAmino replacements for arsine, antimony and phosphine199278
JP H05251339 ASemiconductor substrate and its manufacture—22
US 5,270,247 AAtomic layer epitaxy of compound semiconductor1993157
US 5,273,930 AMethod of forming a non-selective silicon-germanium epitaxial film1993126
US 5,290,824 APhotocrosslinked second order nonlinear optical polymers199421
US 5,366,953 AMethod of forming grain boundary junctions in high temperature superconductor films1994243
US 5,462,603 ASemiconductor processing apparatus1995164
US 5,480,818 AMethod for forming a film and method for manufacturing a thin film transistor1996348
US 5,597,609 AProcess and apparatus for the continuous or semi-continuous coating of eyeglass lenses199732
US 5,616,208 AVacuum processing apparatus, vacuum processing method, and method for cleaning the vacuum processing apparatus1997211
EP 0,794,568 A2Blanket-selective deposition of cvd aluminum and reflectivity improvement using a self-aligning ultra-thin layer—8
US 5,878,458 AElectronic card lock cleaner199926
US 5,916,365 ASequential chemical vapor deposition1999819
US 5,937,300 ASemiconductor apparatus and fabrication method thereof199940
US 5,997,588 ASemiconductor processing system with gas curtain1999111
US 6,060,383 AMethod for making multilayered coaxial interconnect structure200071
US 6,066,358 ABlanket-selective chemical vapor deposition using an ultra-thin nucleation layer200045
US 6,083,832 AMethod of manufacturing semiconductor device200024
US 6,114,099 APatterned molecular self-assembly2000130
US 6,139,695 AModular deposition system having batch processing and serial thin film deposition200054
US 6,142,059 AMethod and apparatus for sensing the orientation of a mechanical actuator200052
US 6,165,916 AFilm-forming method and film-forming apparatus200052

Non-Patent Literature (5)

  • Aarik et al. "Effect of Growth Conditions on Formation of TIO2-II Thin Films in Atomic Layer Deposition Process", Journal of Crystal Growth, vol. 181, Aug. 1997, pp. 259-264.
  • Aarik, et al, "Control of Thin Film Structure by Reactant Pressure in Atomic Layer Deposition of TiO<SUB>2</SUB>", Journal of Crystal Growth, 169 (1996) pp. 496-502.
  • George, et al., "Surface Chemistry for Atomic Layer Growth", Journal of Physical Chemistry, vol. 100, No. 31, pps. 13121-13131, Aug. 1, 1996.
  • Kiyoko et al., Patent Abstract Application No. 04-024917 (JP 9224917, Sep. 1993), "Semiconductor Substrate and Its Manufacture".
  • Ritala, et al., "Atomic Layer Epitaxy-A Valuable Tool for Nanotechnology?" Nanotechnology, vol. 10, No. 1, pps. 19-24, Mar. 1999.