Abstract

A composite structure ( 62 ) having a bond enhancement member ( 76 ) extending across a bond joint ( 86 ) between a ceramic matrix composite (CMC) material ( 80 ) and a ceramic insulation material ( 82 ), and a method of fabricating such a structure. The bond enhancement member may extend completely through the CMC material to be partially embedded in a core material ( 84 ) bonded to the CMC material on an opposed side from the insulation material. A mold ( 26 ) formed of a fugitive material having particles ( 18 ) of a bond enhancement material may be used to form the CMC material. A two-piece mold ( 38, 46 ) may be used to drive a bond enhancement member partially into the CMC material. A compressible material ( 56 ) containing the bond enhancement member may be compressed between a hard tool ( 60 ) and the CMC material to drive a bond enhancement member partially into the CMC material. A surface ( 98 ) of a ceramic insulation material ( 92 ) having a bond enhancement member ( 96 ) extending therefrom may be used as a mold for laying up a CMC material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 46 · Forward citations: 0.

Claims (3)

  1. Claim 1Independent Claim

    A method of fabricating a composite structure, the method comprising: partially embedding a bond enhancement element into a ceramic matrix composite material; applying a ceramic coating to the ceramic matrix composite material over that portion of the bond enhancement element not embedded in the ceramic matrix composite material; and further comprising forming an opening in the ceramic matrix composite material to receive the bond enhancement element.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising forming the opening in the ceramic matrix composite material when the ceramic matrix composite material is in a bisque fired stage.

  3. Claim 3Depends on #1

    The method of claim 1 , further comprising co-firing the ceramic matrix composite material and the ceramic coating to interlock the bond enhancement element there between.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗