US 6,982,012 B2#7244805 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing steel sheet having excellent workability and shape accuracy

13Forward Citations (#7244805 Global)
0.7/yrCitation Velocity (#12162420 Global)
4.46Citation PageRank (#3985484 Global)
11Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of manufacturing a high strength steel sheet containing, in mass %, C: 0.02 to 0.04%, Si: at most 0.4%, Mn: 0.5-3.0%, P: at most 0.15%, S: at most 0.03%, Al: at most 0.50%, N: at most 0.01%, and Mo: 0.01-1.0%. The method includes performing hot rough rolling either directly or after heating to a temperature of at most 1300° C., commencing hot finish rolling either directly or after reheating or holding, completing finish rolling at a temperature of at least 780° C., performing coiling after cooling to a temperature of 750° C. or below at an average cooling rate of at least 3° C./second, heating to an annealing temperature of at least 700° C. and then cooling to a temperature of 600° C. or below at an average cooling rate of at least 3° C./second, then holding in a temperature range of 450-600° C. for at least 10 seconds, and performing hot dip galvanizing after cooling.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a high strength steel sheet comprising casting a slab of steel comprising, in mass %, C: 0.02 to 0.04%, Si: at most 0.4%, Mn: 0.5-3.0%, P: at most 0.15%, S: at most 0.03%, Al: at most 0.50%, N: at most 0.01%, and Mo: 0.01-1.0%, performing hot rough rolling either directly or after heating to a temperature of at most 1300° C., commencing hot finish rolling either directly or after reheating or holding, completing finish rolling at a temperature of at least 780° C., performing coiling after cooling to a temperature of 750° C. or below at an average cooling rate of at le

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗