Abstract
A method and apparatus for controlling a welding-type power supply includes providing a current wave form having an arc current portion and a short circuit current portion. An arc state is entered by retracting a welding wire, and a short circuit state is entered by advancing the wire. The current enters the arc current portion prior to the creation of the arc and the current enters the short circuit current portion prior to the creation of the short, by coordinating the wave form with the wire retraction. This may be preformed on a wire having a diameter of 2.4 mm or more to a weld and applying a welding current of less than 100 amps, or of less than 35 amps. One current waveform during the arc state includes at least three segments, and the last segment is entered into prior to the short circuit state being entered, and is the same current magnitude as the current magnitude at the start of the short circuit state. Penetration and/or bead formation may be controlled by controlling the advancement of the wire into the weld pool. The balance may be user set.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 29.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of controlling a welding-type power supply comprising: providing a current wave form having an arc current portion and a short circuit current portion; causing an arc state to be entered by retracting a welding wire; causing a short circuit state to be entered by advancing the wire; causing the current to enter the arc current portion prior to the creation of the arc by coordinating the wave form with the wire retraction; causing the current to enter the short circuit current portion prior to the creation of the short by coordinating the wave form with the wire advancing.
- Claim 2Depends on #1
The method of claim 1 , further comprising controlling the penetration by controlling the advancement of the wire into the weld pool.
- Claim 3Depends on #1
The method of claim 1 , further comprising controlling bead formation by controlling the advancement of the wire into the w
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 29 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Advantages in using the stick out for increasing the burn off rate in gas metal arc welding: Gerd Huismann 7<SUP>th </SUP>International Symposium of Japan Welding Society (2001) Kobe, Japan.
- An Electrode Vibrator For Vibro-Arc Hardfacing, A.A. Spiridonov, Svar.Proiz., 1966, No. 5, pp. 40-41.
- Calculation of the speed of Movement of the electrode Tip During Welding With mechanical Control of Metal Transfer, V.P. Dmitrienko, Avt. Svarka, 1979, No. 2, pp. 7-9.
- Controlled Mig Short Circuiting Process For Hyperbaric Applications, Gerd Huismann.
- Controlling The Arc Welding Process By Programming the Electrode wire Feed Rate, B.E. Paton, et al., Avt. Svarka, 1977, No. 1, pp. 1-5 and p. 15.