Thin films and method of making them
Abstract
Thin, smooth silicon-containing films are prepared by deposition methods that utilize a silicon-containing precursor. In preferred embodiments, the methods result in Si-containing films that are continuous and have a thickness of about 150 Å or less, a surface roughness of about 5 Å rms or less, and a thickness non-uniformity of about 20% or less. Preferred silicon-containing films display a high degree of compositional uniformity when doped or alloyed with other elements. Preferred deposition methods provide improved manufacturing efficiency and can be used to make various useful structures such as wetting layers, HSG silicon, quantum dots, dielectric layers, anti-reflective coatings (ARC's), gate electrodes and diffusion sources.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 48.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for depositing a thin film, comprising: introducing a gas comprising trisilane to a chamber, wherein the chamber contains a substrate having a surface area of about 300 cm 2 or greater and a substrate surface roughness; establishing trisilane chemical vapor deposition conditions in the chamber; and depositing an amorphous Si-containing film onto the substrate, the amorphous Si-containing film having a thickness in the range of 10 Å to 150 Å and a film surface roughness that is greater than the substrate surface roughness by an amount of about 5 Å rms or less, over a surface area of a
- Claim 2Depends on #1
The method of claim 1 , wherein the amorphous Si-containing film is deposited directly onto a dielectric material.
- Claim 3Depends on #2
The method of claim 2 , wherein the dielectric material is selected from the group consis
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 48 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (3)
- Ikoma et al., Growth of Si/3C-SIC/Si(100) hetrostructures by pulsed supersonic free jets, Applied Physics Letters, vol. 75, No. 25, pp. 3977-3979, Dec. 1999.
- Olivares, J. et al.; "Solid-phase crystallization of amorphous SiGe films deposited by LPCVD on SiO<SUB>2 </SUB>and glass," Thin Solid Films 337 (1999) pp. 51-54.
- Olivares, J. et al.; “Solid-phase crystallization of amorphous SiGe films deposited by LPCVD on SiO2 and glass,” Thin Solid Films 337 (1999) pp. 51-54.