US 6,960,729 B2#22227825 Most CitedExpiredUnited States (USPTO)Utility

Upright-pin-joined resin substrate, method of producing the substrate, pins, and method of producing the pins

5Forward Citations (#22227825 Global)
0.2/yrCitation Velocity (#30554315 Global)
1.22Citation PageRank (#31420280 Global)
15Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

An upright-pin-joined resin substrate 11 includes a resin substrate 13 formed from a resin or a similar material and having a main plane 13 A and a pin pad 17 AP exposed on the main plane; and a number of pins 1 joined to the pin pads 17 AP by means of a solder HD. The pins 1 are obtained by shaping a wire material MT which is formed of 194 Alloy and has been heat-treated in advance at 450° C. to 900° C. The pin 1 includes a shaft portion 1 A and an enlarged-diameter portion 1 B having a round surface projecting in a direction opposite the shaft portion 1 A. The enlarged-diameter portion 1 B and another portion are joined to the pin pad 17 AP through soldering. Also disclosed is a method of producing the upright-pin-joined resin substrate; a pin to be employed in the upright-pin-joined resin substrate; and a method of producing the pin.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An upright-pin-joined resin substrate, comprising: a resin substrate having a plate shape and a main plane, formed from a resin or a resin-containing composite material, and including a pin pad exposed on the main plane; and a pin joined to the pin pad by means of a solder, wherein the pin is formed from a wire material which has been softened through heat treatment prior to formation of the pin, said pin having a shaft portion and an enlarged-diameter portion greater in diameter than the shaft portion, the enlarged-diameter portion being formed at one end of the shaft portion; and at least th

  2. Claim 2Depends on #1

    The upright-pin-joined resin substrate as claimed in claim 1 , wherein the pin is formed from a wire material which has been heat treated at a temperature of from 450° C. to 900° C

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Japanese Office Action for Japanese Patent Application No. 2001-228135 dated Apr. 13, 2004.