A solder joint or seal attaching components having dissimilar coefficients of thermal expansion is made thin (e.g., less than 20 μm and preferably about 5 μm) and of a solder such as an indium-based solder that has a tendency to creep. The solder is toroidal or otherwise shaped to avoid tensile stress in the solder. Axial shearing stress in the solder causes reversible creep without causing failure of the joint or seal. In one embodiment, a toroidal solder seal has a diameter, a footprint, and a thickness in approximate proportions of 5000:200:1.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A solder joint comprising: first and second components having different coefficients of thermal expansion; and solder between and attached to the first and second components, wherein the solder has a toroidal shape and surrounds a cavity formed between the first and second components, and the solder is an indium based alloy that is 48% tin by weight.

  2. Claim 2Depends on #1

    The solder joint of claim 1 , wherein the solder has a stress rupture life of less than about 1,000 minutes at an applied stress of 5 MN·m −2 at an operating temperature of the solder joint.

  3. Claim 3Depends on #1

    The solder joint of claim 1 , wherein the toroidal shape is such that thermal expansion of the first and second components fails to cause significant tensile or tangential stress in the solder.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 3,823,468 AMethod of fabricating an hermetically sealed container197423
GB 2,036,794 ASolder Preform—11
US 4,709,122 ANickel/indium alloy for use in the manufacture of a hermetically sealed container for semiconductor and other electronic devices198730
US 5,050,034 APressure sensor and method of manufacturing same199170
US 5,064,782 AMethod of adhesively and hermetically sealing a semiconductor package lid by scrubbing199164
US 5,168,344 ACeramic electronic package design199261
US 5,248,853 ASemiconductor element-mounting printed board199357
US 5,256,370 ALead-free alloy containing tin, silver and indium199396
US 5,329,160 ASemiconductor package with metalized portions199443
JP H07254840 ASurface acoustic wave device—5
US 5,256,370 B1Lead-free alloy containing tin silver and indium199677
US 5,821,161 ACast metal seal for semiconductor substrates and process thereof199877
US 6,195,478 B1Planar lightwave circuit-based optical switches using micromirrors in trenches2001146
US 6,259,608 B1Conductor pattern for surface mount devices and method therefor200196
US 6,324,316 B1Fabrication of a total internal reflection optical switch with vertical fluid fill-holes200167
US 6,459,160 B1Package with low stress hermetic seal200219
GB 2,379,630 AHollow solder structure and its method of manufacture—3
US 6,627,814 B1Hermetically sealed micro-device package with window2003100
US 6,713,862 B2Low temperature co-fired ceramic-metal packaging technology200439
US 6,848,610 B2Approaches for fluxless soldering200533

Non-Patent Literature (2)

  • Humpston, Giles and Jacobson, David M., "Principles of Soldering and Brazing", ASM International, Materials Park, Ohio, pp. 123-127 (Mar. 1993).
  • Koehler, Dale R. et al., " Ultraminiature Resonator Accelerometer" Sandia Report SAND96-0971, UC-700 (Apr. 1996).