Patents
US 6,953,501 B2#7126895 Most CitedExpiredUnited States (USPTO)Utility

Wood treatment composition and method of use

14Forward Citations (#7126895 Global)
0.7/yrCitation Velocity (#11417934 Global)
1.76Citation PageRank (#17777009 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A wood treatment composition for the preservation of wood comprises a mixture of creosote and a polymer which is miscible with the creosote at about 200° F. and does not substantially phase-separate when the wood treatment composition is under ambient conditions. The polymer may include, but is not limited to, ethylene vinyl acetate copolymers, ethylene methyl acrylate copolymers, ethylene ethyl acrylate copolymers, ethylene butyl acrylate copolymers, ethylene acrylic acid copolymers, ethylene methacrylic acid copolymers, ethylene methyl methacrylic acid copolymers, ethylene styrene interpolymers, styrene acrylic acid copolymers, styrene methacrylic acid copolymers, styrene methyl acrylate copolymers, styrene butadiene styrene block copolymers, styrene ethylene butylene styrene block copolymers, or a blend thereof. Preferably, the creosote is present in an amount of at least 50 percent by weight of the composition. Such compositions can be used to treat wood surfaces to prolong the service life of the wood.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 14.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A wood treatment composition, comprising: a mixture of creosote and a thermoplastic polymer having a melting point or a glass transition temperature below about 210.degree. F. which is miscible with the creosote at about 200° F. and does not substantially phase-separate when the wood treatment composition is under ambient conditions, and the creosote is present in an amount of at least 50 percent by weight of the composition.

  2. Claim 2Depends on #1

    The wood treatment composition of claim 1 , wherein the polymer has a melt index higher than about 50 g/10 min.

  3. Claim 3Depends on #1

    The wood treatment composition of claim 1 , wherein the polymer has a melt index higher than about 200 g/10 min.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Search, Report, Nov. 6, 2002.