Abstract

This invention relates to a surface treatment method comprising the steps of providing a treating solution containing a specific ammonium compound or aqueous ammonia, and magnesium silicofluoride, heating the treating solution to a temperature of 70 to 100° C., and soaking aluminum or an aluminum alloy in the treating solution; a piston having a surface coated with a film consisting of a mixture of NH 4 MgAlF 6 and MgAlF 5 .1.5H 2 O or a mixture of NH 4 MgAlF 6 and MgAl 2 F 8 .2H 2 O; and a sliding member made of aluminum or the like wherein the whole surface of the sliding member or the sliding surface thereof is coated with a film which consists of either of the aforesaid mixtures, has a cubic crystal structure, and shows no crystalline orientation. The present invention can provide a surface treatment method which requires simple equipment, can reduce treatment costs, and can yield aluminum or an aluminum alloy having excellent abrasion resistance, corrosion resistance and other properties, as well as sliding members and pistons having excellent abrasion resistance and other properties.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An aluminum or an aluminum alloy piston having undergone a surface treatment comprising the steps of providing a treating solution containing an ammonium compound selected from the group consisting of ammonium borofluoride, ammonium chloride and aqueous ammonia, and magnesium silicofluoride; heating the treating solution to a temperature of 70 to 100° C.; and soaking said aluminum or an aluminum alloy piston in the treating solution.

  2. Claim 2Independent Claim

    A piston having a surface coated with a film comprising a mixture of NH 4 MgAlF 6 and MgAlF 5 .1.5H 2 O or a mixture of NH 4 MgAlF 6 and MgAl 2 F 8 .2H 2 O.

  3. Claim 3Depends on #2

    The piston according to claim 2 wherein its whole surface including the piston ring grooves, piston pin boss, skirt, piston head and internal piston surface is coated with the film comprising the mixture of NH 4 MgAlF 6 and MgAlF 5 .1.5H 2 O or the mi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (1)

  • English translation of Dec. 27, 2004 Office Action corresponding to Japanese Patent Application No. 2000-116253.