hottubpatentshottub.tech
US 6,940,220 B2#134507 Most CitedExpiredUnited States (USPTO)Utility

Glass, method for its production, and FED device

0Forward Citations (#134507 Global)
0.0/yrCitation Velocity (#134507 Global)
0.98Citation PageRank (#134507 Global)
8Prior Art Cited
19Structured Claims
0Drawings / Sheets

Abstract

Glass comprises essentially 20-70% SiO 2 , 10-50% TiO 2 +Nb 2 O 5 +SnO 2 +Ta 2 O 5 +WO 3 +CeO 2 , 0-50% MgO+CaO+SrO+BaO+ZnO, and 0-30% B 2 O 3 +Al 2 O 3 , in molar percentage terms based on the oxides; and has a resistivity of at most 10 15 Ω·cm at 20° C. A method for production of glass is to produce the glass under such a condition that a redox represented by [Fe 2+ ]/([Fe 2+ ]+[Fe 3+ ]) where Fe is present in the glass, is at least 0.6.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 0.

Claims (19)

  1. Claim 1Independent Claim

    A glass comprising 20-70% SiO 2 , 10-50% TiO 2 +Nb 2 O 5 +SnO 2 +Ta 2 O 5 +WO 3 +CeO 2 , at least 10% BaO, and up to 50% MgO+CaO+SrO+BaO+ZnO, and 0-30% B 2 O 3 +Al 2 O 3 , in molar percentage terms based on the oxides; and having a resistivity of at most 10 15 Ω·cm at 20° C.

  2. Claim 2Depends on #1

    The glass according to claim 1 , which comprises 10-50 mol% Nb 2 O 5 .

  3. Claim 3Depends on #1

    The glass according to claim 1 , which contains La 2 O 3 and/or Y 2 O 3 in a total amount of at most 15 mol %.

  4. Claim 4Depends on #1

    The glass according to claim 1 , which has a glass transition point of at least 500° C.

  5. Claim 5Independent Claim

    A method for production of glass comprising melting raw materials which are prepared so as to obtain a glass comprising 20-70% SiO 2 , 10-50% TiO 2 +Nb 2 O 5 +SnO 2 +Ta 2 O 5 +WO 3 +CeO 2 , 0-50% MgO+CaO+SrO+BaO+ZnO, and 0-30% B 2 O 3 +Al 2 O 3 , in molar percentage terms based on the oxides, and having a resistivity of at most 10 15 Ω·cm at 20° C., wherein the glass is produced under such a condition that a redox R represented by [Fe 2+ ]/([Fe 2+ ]+[Fe 3+ ]) where Fe is present in the glass, is at least 0.6.

  6. Claim 6Depends on #5

    The method for production of glass according to claim 5 , wherein the R is measured under the condition that a content of Fe as Fe 2 O 3 is 0.01-1.0 mol %.

  7. Claim 7Depends on #5

    The method for production of glass according to claim 5 , wherein the glass contains La 2 O 3 and/or Y 2 O 3 in a total amount of at most 15 mol %.

  8. Claim 8Depends on #5

    A glass produced by the method as defined in claim 5 .

  9. Claim 9Independent Claim

    A field emission display device comprising an anode panel having a phosphor, an emitter panel having an emitter for emitting an electron, and a plurality of spacers, the anode panel and the emitter panel facing each other through the spacers, wherein the spacers are a glass comprising 20-70% SiO 2 , 10-50% TiO 2 +Nb 2 O 5 +SnO 2 +Ta 2 O 5 +WO 3 +CeO 2 , 10-50% MgO+CaO+SrO+BaO+ZnO, and 0-30% B 2 O 3 +Al 2 O 3 , in molar percentage terms based on the oxides; and having a resistivity of at most 10 15 Ω·cm at 20° C.

  10. Claim 10Independent Claim

    A device comprising a glass, the glass comprising 20-70% SiO 2 , 10-50% TiO 2 +Nb 2 O 5 +SnO 2 +Ta 2 O 5 +WO 3 +CeO 2 , 0-50% MgO+CaO+SrO+BaO+ZnO, and 0-30% B 2 O 3 +Al 2 O 3 , in molar percentage terms based on the oxides; and having a resastivity of at most 10 15 Ω·cm at 20° C., wherein the device is selected from the group consisting of electrodes, thermistor sensors, reactors, and switching-material micro-electro-mechanical systems.

  11. Claim 11Depends on #1

    The glass according to claim 1 , which has a resistivity of at most most 10 14 Ω·cm at 20° C.

  12. Claim 12Depends on #1

    The glass according to claim 1 , which has a resistivity of at most most 10 13 Ω·cm at 20° C.

  13. Claim 13Depends on #1

    The glass according to claim 1 , which has a resistivity of at most most 10 12 Ω·cm at 20° C.

  14. Claim 14Depends on #1

    The glass according to claim 1 , which has an average linear expansion coefficient α of 60×10 −7 -110×10 −7 /° C. in a range of 50-350° C.

  15. Claim 15Depends on #4

    The glass according to claim 4 , which has a glass transition temperature of at least 700° C.

  16. Claim 16Depends on #15

    The glass according to claim 15 , which has a glass transition temperature of at least 740° C.

  17. Claim 17Depends on #1

    The glass according to claim 1 , wherein SiO 2 is present in an amount of 30-60%, TiO 2 +Nb 2 O 5 +SnO 2 +Ta 2 O 5 +WO 3 +CeO 2 is present in an amount of 15-45%, MgO+CaO+SrO+BaO+ZnO is present in an amount of 15-45%, and B 2 O 3 +Al 2 O 3 is present in an amount of 0-25%, in molar percentage terms based on the oxides.

  18. Claim 18Depends on #1

    The glass according to claim 1 , wherein Li 2 O, Na 2 O, and K 2 O are present in an amount of 0-5%, in molar percentage terms based on the oxides.

  19. Claim 19Depends on #3

    The glass according to claim 3 , wherein La 2 O 3 and/or Y 2 O 3 are present in a t

Technical Overview & Description

TECHNICAL FIELD The present invention relates to a glass having a low resistivity, a method for its production, and a field emission display device (hereinafter, referred to as “FED”). BACKGROUND ART An FED is a cathode-ray tube (CRT) panel having a large number of microscopic electron guns of micron size arranged corresponding to each of pixels. Since the FED, in which the electron guns are driven in each of the pixels independently of each other, requires no scan of an electron beam over a wide angle range unlike the CRT panels, it is a display far thinner and flatter than the CRT panels (e.g., reference should be made to JP-A-07-230776). Particularly, the FED is expected as a large-screen flat display of at least 40 inches, which is hardly realized by the CRT panels. In the FED, an anode panel with phosphors faces an emitter panel with emitters for emitting electrons, through a plurality of spacers, and the periphery of the anode panel and emitter panel is sealed with a glass paste or the like. The internal space of FED, i.e., the space between the anode panel and the emitter panel facing each other is typically in a high vacuum state of 10 −3 −10 −5 Pa, and electrons emitted from an emitter of the emitter panel into the space impinge upon a phosphor of the anode panel to induce electron beam induced luminescence. As a result, a pixel to which the phosphor belongs develops a color. The distance between the anode panel and the emitter panel facing each other is typically 1-2 mm, and, in order to keep the distance independently of the pressure difference between the atmospheric pressure and the pressure of the internal space (e.g., 10 −3 −10 −5 Pa), the spacers are interposed between the anode panel and the emitter panel, as described above. The conventional spacers were made of alumina. The spacers of alumina were likely to be charged with electrons, which raised the problem that the display image tended to be dist

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (8)

PatentTitleYearCitations