Patents
US 6,939,754 B2#15829665 Most CitedExpiredUnited States (USPTO)Utility

Isotropic polycrystalline silicon and method for producing same

7Forward Citations (#15829665 Global)
0.3/yrCitation Velocity (#22887529 Global)
1.52Citation PageRank (#22465485 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A high-quality isotropic polycrystalline silicon (poly-Si) and a method for fabricating high quality isotropic poly-Si film are provided. The method includes forming a film of amorphous silicon (a-Si) and using a MISPC process to form poly-Si film in a first area of the a-Si film. The method then anneals a second area, included in the first area, using a Laser-Induced Lateral Growth (LILaC) process. In some aspects, a 2N-shot laser irradiation process is used as the LILaC process. In some aspects, a directional solidification process is used as the LILaC process. In response to using the MISPC film as a precursor film, the method forms low angle grain boundaries in poly-Si in the second area.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 7.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for producing high quality isotropic polycrystalline silicon (poly-Si), the method comprising: forming a film of amorphous silicon (a-Si); using a metal induced solid phase crystallization (MISPC) process to form poly-Si film in a first area of the a-Si film; and, annealing a second area, included in the first area, using a Laser-Induced Lateral Growth (LILaC) process selected from a group including a 2N-shot and a directional solidification (DS) process.

  2. Claim 2Depends on #1

    The method of claim 1 wherein using a MISPC process to form poly-Si film in the first area includes: overlying a first area top surface with a nucleating site forming material; selected from the group including cobalt, copper, gold, iron, nickel palladium, and platinum; and, having a thickness in a range of 10 to 80 angstroms (A); and, heating the amorphous silicon film and the film of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • J.S. Im and H.J. Kim, Appl. Phys. Lett., 63, 1969 (1993).
  • J.S. Im, Phys. Stat. Sol. A, 166, 603 (1998).
  • R. Sposili and J.S. Im, Appl. Phys. Lett., 69, 2864 (1996).