Accelerated method to determine or predict failure time in polyethylenes
Abstract
An accelerated method of determining the failure time of a polyethylene resin by determining the minimum displacement rate, or the time at minimum displacement rate, using ASTM F 1473-01, then following one of these routes: (1) If failure has not yet occurred, cryogenically fracturing the resin specimen and examining it for slow crack growth to determine whether the anticipated, or desired, failure time is generally before or after the predicted failure time; or (2) Applying the minimum displacement rate, or the time at minimum displacement rate, in the appropriate mathematical formula to predict the failure time for the resin. The mathematical formula is derived from the discovery of a power law relationship between the failure time and minimum displacement rate, or between failure time and the time at minimum displacement rate. Thus, it is not necessary to actually test all the way to failure using ASTM F 1473-01, thereby accelerating testing capability and consequently enabling more rapid development of new resins.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An accelerated method of determining or predicting failure time in polyethylene materials, comprising selecting an anticipated or desired failure time for a polyethylene material specimen; conducting a PENT (Pennsylvania Notched Test) on the specimen according to ASTM F1473-01 for a time equivalent to the time at Min δ R , wherein Min δ R =minimum displacement rate in millimeters and time is measured in hours, that corresponds to the anticipated or desired failure time; and either determining that, (a) if failure has occurred, PENT failure time is before the anticipated or desired failure time
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (6)
Non-Patent Literature (5)
- ASTM International, Designation: D 1598-97, Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure, pp. 24-27.
- ASTM International, Designation: D 2837-01, Standard Test Method for Obtaining Hydrostatic Design Basis for Thermoplastic Pipe Materials, pp. 281-294, 5 Tables.
- ASTM International, Designation: F 1473-01, Standard Test Method for Notch Tensile Test to Measure the Resistance to Slow Crack Growth of Polyethylene Pipes and Resins, pp. 1160-1165, 3 Figs, 1 Table.
- ASTM International, Designation: F 1474-98 (Reapproved 2001), Standard Test Method for Slow Crack Growth Resistance of Notched Polyethylene Plastic Pipe, pp. 1166-1168, 3 Figs.
- ASTM International, Designation: F 3417-99, Standard Test Method for Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry (DSC), 330-333, 2 Figs.