This composite oxide powder can secure a large pore volume even after calcination at high temperature and, when a catalyst is formed by loading a noble metal on this composite oxide powder, noble metal grain growth can be suppressed. The composite oxide powder comprises particles of an oxide of a metal M 1 and an oxide of a metal M 2 which does not dissolve in the oxide of the metal M 1 , the oxide of the metal M 1 and the oxide of the metal M 2 being dispersed at the nanometer level. Since different oxides serve as a barrier to each other, sintering is suppressed. Therefore, in the case of composite oxide powder comprising Ce as a metal M 1 and Al as a metal M 2 , grain growth is small even after exposed to high temperature and pores of 3.5-100 nm secure a volume of 0.07 cc/g or more after calcination at 600° C. for 5 hours and a volume of 0.04 cc/g or more after calcination at 800° C. for 5 hours.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 29.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A composite oxide powder, consisting essentially of: a mixture of particles of an oxide of metal M 1 which is cerium and an oxide of a metal M 2 which is at least one element selected from the group consisting of aluminum, titanium and silicon and which does not dissolve in said oxide of metal M 1 , wherein the cerium oxide constitutes more than 50% by wt of the composite oxide powder said mixture having been calcined at 600° C. for 5 hours or at 800° C. for 5 hours, and wherein the calcination of said mixture when calcined at 600° C for 5 hours results in a composite oxide powder having a p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 29 total)

PatentTitleYearCitations
US 2010227757 A1Inorganic mixed oxide and catalyst for purification of exhaust gas using the same—10
US 11,484,864 B2Exhaust gas-purifying three-way catalyst and method for producing same, and integral structure type exhaust gas-purifying catalyst20222
US 7,354,882 B2Carbon monoxide removing catalyst and production process for the same as well as carbon monoxide removing apparatus20080
US 2007215009 A1Metal Oxide Nanoporous Material, Coating Composition to Obtain the Same, and Methods of Manufacturing Them—23
US 2004234439 A1Porous composite oxide and production method thereof—36
US 2006172886 A1Catalyst support and method of producing the same—21
US 2005090393 A1Novel catalyst for the reduction of NO to N2 with hydrogen under NOx oxidation conditions—6
US 7,935,653 B2Metal oxide nanoporous material, coating composition to obtain the same, and methods of manufacturing them20118
US 2006160697 A1Carbon monoxide removing catalyst and production process for the same as well as carbon monoxide removing apparatus—1
US 7,105,137 B2Catalyst for the reduction of NO to N2 with hydrogen under NOx oxidation conditions200623
US 7,393,808 B2Particulate matter-oxidizing material and oxidizing catalyst200813
US 7,247,597 B2Composite oxide, process for producing the same, and exhaust gas reducing co-catalyst200720
US 8,067,332 B2Methanation catalyst, and carbon monoxide removing system, fuel processor, and fuel cell including the same20113
US 2007259975 A1Methanation catalyst, and carbon monoxide removing system, fuel processor, and fuel cell including the same—11
US 8,574,524 B2Porous composite oxide and production method thereof20132