Lithium cobalt oxides and methods of making same

11Forward Citations (#9140976 Global)
0.5/yrCitation Velocity (#15066157 Global)
2.55Citation PageRank (#9852385 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention includes lithium cobalt oxides having hexagonal layered crystal structures and methods of making same. The lithium cobalt oxides of the invention have the formula Li w Co 1−x A x O 2+y wherein 0.96≦w≦1.05, 0≦x≦0.05, −0.02≦y≦0.02 and A is one or more dopants. The lithium cobalt oxides of the invention preferably have a position within the principal component space defined by the relationship ax i +by i ≦c, wherein x i ={right arrow over (S)} i •{right arrow over (P)} c1 ; y i ={right arrow over (S)} i •{right arrow over (P)} c2 ; the vector {right arrow over (S)} i is the x-ray spectrum for the Li w Co 1−x A x O 2+y compound; the vectors {right arrow over (P)} c1 and {right arrow over (P)} c2 defining the principal component space are determined by measuring the x-ray powder diffraction values {right arrow over (S)} i between 15° and 120° using a 0.02° step size and CuKα rays for a large sample set of lithium cobalt oxides and using the regression of {right arrow over (S)} i of the sample set against the capacity fade after 50 cycles of a lithium coin cell that includes a lithium negative electrode and the lithium cobalt oxide as the positive electrode material

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 11.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a lithium cobalt oxide Li w Co 1−x A x O 2+y having a hexagonal layered crystal structure wherein 0.96≦w≦1.05, 0≦x≦0.05, −0.02≦y≦0.02 and A is one or more dopants, comprising the steps of: heating a lithium source compound, a cobalt source compound, and optionally one or more source compounds containing dopants A in a rotary calciner at a temperature below about 850° C. to produce Li w Co 1−x A x O 2+y ; heating the Li w Co 1−x A x O 2+y compound in a rotary calciner at a temperature from about 900° C. to 1000° C. to refine the hexagonal layered crystal structure; and

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein said first heating step comprises heating the source compounds at a temperature of from about 500° C. to about 85

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (11 of 11 total)

PatentTitleYearCitations
US 2009075175 A1Lithium metal composite oxide particles, process of producing lithium metal composite oxide particles, electrode structure containing lithium metal composite oxide particles, process of producing electrode structure , and lithium secondary battery having electrode structure—1
US 2004175618 A1Lithium metal composite oxide particles, process of producing lithium metal composite oxide particles, electrode structure containing lithium metal composite oxide particles, process of producing electrode structure, and lithium secondary battery having electrode structure—56
US 2010310936 A1Cathode active material, cathode and nonaqueous secondary battery—9
US 2011064980 A1Cathodic active material , cathode, and nonaqueous secondary battery—8
US 7,510,805 B2Lithium metal composite oxide particles having particles with columnar or planar shape20092
US 7,927,743 B2Lithium metal composite oxide particles, process of producing lithium metal composite oxide particles, electrode structure containing lithium metal composite oxide particles, process of producing electrode structure, and lithium secondary battery having electrode structure20114
US 2004142241 A1Method of producing positive electrode active material for non-aqueous electrolyte secondary battery—16
US 2010124703 A1Cathode active material, cathode, and nonaqueous secondary battery—12
US 7,157,186 B2Method of producing positive electrode active material for non-aqueous electrolyte secondary battery20075
US 2010143801 A1Lithium metal composite oxide particles, process of producing lithium metal composite oxide particles, electrode structure containing lithium metal composite oxide particles, process of producing electrode structure , and lithium secondary battery having electrode structure—3
US 7,682,595 B2Process of producing lithium metal composite oxide particles20100

Non-Patent Literature (5)

  • A. De Kock, E. Ferg and R.J. Gummow; The effect of multivalent cation dopants on lithium manganese spinel cathodes; Journal of Power Sources 70, pp. 247-252, (1998).
  • A. Van Der Ven, M.K. Aydinol, G. Ceder, G. Kresse and J. Hafner; First-principles investigation of phase stability in Li<SUB>x</SUB>CoO<SUB>2</SUB>; 1998 The American Physical Society, vol. 58; No. 6, pp. 2975-2987.
  • A. Van Der Ven, M.K. Aydinol, G. Ceder, G. Kresse and J. Hafner; First-principles investigation of phase stability in LixCoO2; 1998 The American Physical Society, vol. 58; No. 6, pp. 2975-2987.
  • A.K. Padhi, W.B. Archibald, K.S. Nanjundaswamy and J.B. Goodenough; Ambient and High-Pressure Structures of LiMnVO<SUB>4 </SUB>and Its Mn<SUP>3+</SUP>/Mn<SUP>2+ </SUP>Redox Energy; Journal of Solid State Chemistry 128, Article No. SC967217, pp. 267-272 (1997).
  • A.K. Padhi, W.B. Archibald, K.S. Nanjundaswamy and J.B. Goodenough; Ambient and High-Pressure Structures of LiMnVO4 and Its Mn3+/Mn2+ Redox Energy; Journal of Solid State Chemistry 128, Article No. SC967217, pp. 267-272 (1997).