Patents
US 6,932,142 B2#85222778 Most CitedExpiredUnited States (USPTO)Utility

Reduction casting method

0Forward Citations (#85222778 Global)
0.0/yrCitation Velocity (#85222778 Global)
0.56Citation PageRank (#85222778 Global)
5Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A reduction casting method includes the steps of: pouring a molten metal into a cavity of a molding die; and performing casting while reducing an oxide film formed on a surface of the molten metal by allowing the molten metal and a reducing substance to come into contact with each other in the cavity. On this occasion, the molten metal is poured into the cavity in a state in which the molding die is forcibly cooled by a cooling device, thereby being rapidly cooled. Further, on this occasion, a solidification speed at which the molten metal is rapidly cooled is allowed to be 600° C./min or more. Still further, on this occasion, the molten metal is filled into the cavity in a filling time of from 1.0 second to 9.0 seconds.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A reduction casting method, comprising the steps of: pouring a molten metal into a cavity of a molding die in a state in which the molding die is forcibly cooled by a cooling device, whereby the molten metal is rapidly cooled; and performing casting while reducing an oxide film formed on a surface of the molten metal by allowing the molten metal and a reducing substance to come into contact with each other in the cavity, wherein a solidification speed at which the molten metal is rapidly cooled is set to be 600° C./min or more; and wherein the molten metal is filled into the cavity in a fillin

  2. Claim 2Depends on #1

    The reduction casting method as set forth in claim 1 , wherein a DASII value is allowed to be 22 μm or less by setting the solidification speed of the molten metal to be 600° C./min or more.

  3. Claim 3Independent Claim

    The

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • European Search Report dated May 19, 2004.