Patents
US 6,930,399 B2#9645311 Most CitedExpiredUnited States (USPTO)Utility

High reliability non-conductive adhesives for non-solder flip chip bondings and flip chip bonding method using the same

11Forward Citations (#9645311 Global)
0.5/yrCitation Velocity (#15105625 Global)
1.68Citation PageRank (#19237185 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The method of the present invention comprises the steps of: providing an IC chip having I/O pads, each having a non-solder bump such as Au or Cu stud bump or Ni\Cu\Au bump formed thereon, and a substrate having metal electrodes formed thereon; applying a film-type non-conductive adhesive (NCA) to the chip or substrate, the adhesive including solid-phase bisphenol A type epoxy resin, liquid-phase bisphenol F type epoxy resin, solid-phase phenoxy resin, methylethylketone/toluene solvent, liquid-phase hardener, and non-conductive particles; and thermo-compressing the IC chip to the substrate so that the non-solder bump and the metal electrode can be mechanically and electrically connected. The NCA of the present invention has high reliability since it has lower thermal expansion coefficient and dielectric constant than conventional NCAs and has excellent mechanical and electrical characteristics. In addition, the NCA can be effectively selected at need and applied to diverse processes since it can be made to a form of paste rather than film. The method of the present invention is harmless to the environment since it does not employ conventional solder bumps using solder as a chief ing

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 11.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Non-conductive adhesive for flip chip bonding that is dried and has the form of a film, comprising: 6˜10 wt % of solid-phase bisphenol A type epoxy resin; 15˜25 wt % of liquid-phase bisphenol F type epoxy resin; 12˜18 wt % of solid-phase phenoxy resin; 32˜40 wt % of solvent mixture with methylethylketone and toluene with the ratio of 1:3 in vol %; 8˜14 wt % of liquid-phase imidazole hardener; and 6˜20 wt % of non-conductive SiO2 or SiC particles.

  2. Claim 2Depends on #1

    Non-conductive adhesive for flip chip bonding of claim 1 , wherein the thickness of the film is 10˜50 μm.

  3. Claim 3Depends on #1

    Non-conductive adhesive for flip chip bonding of claim 1 , wherein an epoxy adhesion enhanced layer with the thickness of 2˜5 μm, the epoxy adhesion enhanced layer being made by mixing 6˜10 wt % of solid-phase bisphenol A type epoxy resin, 15˜25 wt % of liquid-phase bisphe

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • English language abstract of Korean Patent Publication No. 1020000046722.
  • English language abstract of Korean Patent Publication No. 1997-0061017.