Abstract

1-butene based polymer satisfying following requirements (1″) to (4″) provides formed product having low stickiness, superior flexibility and transparency. (1″) Crystalline resin having melting point (Tm−P), not observed or in the range of 0 to 100° C., wherein said melting point defined as the peak top of the peak observed in the highest temperature zone of the melting heat absorption curve obtained by heating a sample of said polymer at a rate of 10° C./minute using Differential Scanning Calorimeter (DSC), after melting said sample in advance at 190° for 5 minutes under nitrogen atmosphere, followed by cooling it to −10° C. at a rate of 5° C./minutes, and keeping it at −10° C. for 5 minutes. (2″) Stereoregularity index {(mmmm)/(mmrr+rmmr)} is at most 20. (3″) Molecular weight distribution (Mw/Mn) measured by Gel Permeation Chromatography (GPC) method is at most 4.0. (4″) Weight average molecular weight (Mw) measured by GPC method is in the range of 10,000 to 1,000,000.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 18.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A 1-butene based polymer which satisfies the following: (1) it is a crystalline resin having a melting point (Tm−D) in the range of 0 to 100° C., wherein the melting point is defined as the peak top of the peak observed in the highest temperature zone of the melting heat absorption curve obtained by heating a sample of the polymer at a rate of 10° C./minute using the Differential Scanning Calorimeter (DSC), after keeping said sample in advance at −10 ° C. for 5 minutes under a nitrogen atmosphere, (2) it has a stereoregularity index {(mmmm)/(mmrr+rmmr)} which is at most 20, (3) it has a molecu

  2. Claim 2Independent Claim

    A 1-butene based polymer which sat

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Longo et al., "13C-Enriched End Groups of Isotactic Polypropylene and Poly(1-butene) Prepared in the Presence of Ethylenediindenyldimethyltitanium and Methylalumoxane", Macromolecules 1987, 20, 1015-1018.