Conductive metal particles, conductive composite metal particles and applied products using the same

8Forward Citations (#13885581 Global)
0.4/yrCitation Velocity (#21170691 Global)
1.50Citation PageRank (#22757805 Global)
23Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Disclosed are provides conductive metal particles and conductive composite metal particles by which conductive materials having stable conductivity can be provided, and applied product thereof. The conductive metal particles have a number average particle diameter of 5 to 100 μm, a BET specific surface area of 0.01×10 3 to 0.7×10 3 m 2 /kg, a sulfur element content of at most 0.1% by mass, an oxygen element content of at most 0.5% by mass and a carbon element content of at most 0.1% by mass. The conductive composite metal particles are obtained by coating the surfaces of the conductive metal particles with a high-conductive metal.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Conductive composite metal particles obtained by coating the surfaces of conductive metal particles with a high-conductive metal, wherein the conductive metal articles are formed from a metallic material selected from the group consisting of iron, nickel, cobalt and alloys thereof, having a number average particle diameter of 5 to 100 μm a BET specific surface area of 0.01×10 3 to 0.7×10 3 m 2 /kg, a sulfur element content of at most 0.1% by mass, an oxygen element content of at most 0.5% by mass and a carbon element content of at most 0.1% by mass, and wherein the coefficient of variation o

  2. Claim 2Depends on #1

    The conductive composite metal particles according to claim 1 , wherein the thickness t of the coating layer of the high-conductive metal, which is calculated

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (23)

PatentTitleYearCitations
US 3,983,075 ACopper filled conductive epoxy197646
US 4,450,188 AProcess for the preparation of precious metal-coated particles198463
US 4,455,167 ANickel-zinc dust-iron-nickel powder pigment system198410
US 4,579,882 AShielding material of electromagnetic waves198651
US 4,600,604 AMetal oxide-coated copper powder198634
US 4,687,597 ACopper conductor compositions198727
US 4,711,814 ANickel particle plating system198743
US 4,729,809 AAnisotropically conductive adhesive composition1988105
US 4,776,980 AInductor insert compositions and methods198871
US 4,828,613 APowdery raw material for manufacturing anodes of fuel cells19897
US 4,833,033 AResin coated copper powder for electroconductive paints198921
US 4,857,233 ANickel particle plating system198927
US 4,944,797 ALow oxygen content fine spherical copper particles and process for producing same by fluid energy milling and high temperature processing199028
US 5,068,150 ACopper powder for electroconductive paints and electroconductive paint compositions199128
US 5,180,513 AShielded plastic enclosure to house electronic equipment199346
US 5,584,908 AMicron-sized nickel metal powder and a process for the preparation thereof199629
JP H10188672 AConductive elastomer composition—9
JP H10204223 AComposition for conductive elastomer—3
JP H11134936 AConductive fine grains, anisotropic conductive adhesive, and conductive connecting structure—8
US 5,968,225 AHydrogen storage alloy powder and an electrode comprising the same19993
US 6,036,839 ALow density high surface area copper powder and electrodeposition process for making same200026
US 6,381,419 B1Image forming apparatus with developer density and developer remaining amount detection features200221