Abstract

TiAl alloy includes 46 to 50 at % of Al, 5 at % or less of combination of Mo, V and Si, provided that Si content is 0.7 at % or less, and Mo content satisfies an equation of −0.3x +17.5 at % or less where x represents Al (at %), and the remainder being Ti and inevitable impurities. Mo may be replaced by Fe or combination of Mo and Fe. TiAl alloy is heated to a melt, poured into a mold, and cooled at a rate of 150 to 250° C./min within a temperature range of 1500 to 1100° C. The resulting product can be used as cast. If desired, however, heat treatment such as HIP or homogenization may be performed within a temperature range of 1100 to 800° C. After the heat treatment, the melt is cooled at a rate of 100° C./min or more until room temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 3.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A casting method comprising the steps of: A) preparing a TiAl alloy having the following composition: Al: 46 to 50 at % Mo, V and Si: each individually being present and a total of these elements being greater than 0 and less than or equal to 5 at %, provided that Si content is greater than 0 and less than or equal to 0.7 at %, and Mo content satisfies an equation of −0.3x+17.5 at % or less where x represents Al (at %), and the remainder being Ti and inevitable impurities; B) heating the TiAl alloy to a melt; C) pouring the melt into a mold; and D) cooling the melt at a rate of 150 to 250° C./

  2. Claim 2Independent Claim

    A casting method comprising the steps of: A) preparing a TiAl alloy having the following composition: Al: 46 to 50 at %, Fe, V and Si: a total of these elements

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Kim, M.C. et al: "Composition and growth rate effects in directionally solidified TiAl alloys", Material Science and Engineering, (1997), A239-240, pp. 570-576.
  • Kimura, M. et al: "Study on phase stability in Ti-Al-X systems at high temperatures", Material Science and Engineering, (1992), A152, pp. 54-59.
  • Knippscheer, S. et al: "Intermetallic TiAl (Cr,Mo,Si) Alloys for Lightweight Engine Parts. Structure, Properties and Applications", Advanced Engineering Materials, (1999) 1,3-4, pp. 187-191.
  • Singh, A.K. et al: "Transforamtions in ox2 + y Titanium Aluminide Alloys Containing Molybdenum: Part I. Solidification Behavior", Metallurgical and Materials Transactions A, (1997), 28A, pp. 1735-1743.
  • Singh, A.K. et al: "Transformations in ox2 + y Titanium Aluminide Alloys Containing Molybdenum: Part II. Heat Treatment", Metallurgical and Materials Transactions A, (1997), 28A, pp. 1745-1753.