Alloy and method of producing the same
Abstract
In accordance with a preferred embodiment of the invention, an alloy or other composite material is provided formed of a bulk metallic glass matrix with a microstructure of crystalline metal particles. The alloy preferably has a composition of (X a Ni b Cu c ) 100−d−c Y d Al c , wherein the sum of a, b and c equals 100, wherein 40≦a≦80, 0≦b≦35, 0≦c≦40, 4≦d≦30, and 0≦e≦20, and wherein preferably X is composed of an early transition metal and preferably Y is composed of a refractory body-centered cubic early transition metal. A preferred embodiment of the invention also provides a method of producing an alloy composed of two or more phases at ambient temperature. The method includes the steps of providing a metastable crystalline phase composed of at least two elements, heating the metastable crystalline phase together with at least one additional element to form a liquid, casting the liquid, and cooling the liquid to form the alloy. In accordance with a preferred embodiment of the invention, the composition and cooling rate of the liquid can be controlled to determine the volume fraction of the crystalline phase and determine the size of the crystalline particles, respectively.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing an amorphous alloy comprising two or more phases at ambient temperature, comprising the steps of: providing a metastable crystalline alloy comprising at least two elements; heating the metastable crystalline alloy together with at least one additional element to form a liquid with suspended particles of a crystalline phase; casting the liquid; and cooling the liquid to form the amorphous alloy; wherein said providing includes controlling composition of the liquid.
- Claim 2Depends on #1
The method of claim 1 , wherein the controlling of the composition of the liquid determines a volume fraction of the metastable crystalline alloy.
- Claim 3Depends on #1
The method of claim 1 , wherein said heating comprises heating the metastable crystalline alloy together with at least two additional elements, the additional elements being combined with each ot
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (24)
Non-Patent Literature (5)
- Fan, C. and Inoue, A.; "Ductility of bulk nanocrystalline composites and metallic glasses at room temperature", Applied Physics Letters, vol. 77, No. 1, pp. 46-48, Jul. 3, 2000.
- Fan, C.; Li, C.; Inoue, A.; Haas, V.; "Deformation behavior of Zr-based bulk nanocrystalline amorphous alloys", Physical Review B (Condensed Matter), vol. 61, No. 6, p. R3761-3, Feb. 1, 2000.
- Hays, C.C., et al., "Microstructure Controlled Shear Band Pattern Formation and Enhanced Plasticity of Bulk Metallic Glasses Containing in situ Formed Ductile Phase Dendrite Dispersons", Physical Review Letters, vol. 84, No. 13, Mar. 28, 2000.
- Kuhn, U., et al., "ZrNbCuNiAl bulk metallic glass matrix composites containing dendritic bcc phase precipitates", Applied Physics Letters, vol. 80, No. 14, Apr. 8, 2002.
- Saida, J.; Inoue, A.; "Icosahedral quasicrystalline phase formation in Zr-Al-Ni-Cu glassy alloys by addition of Nb, Ta and V elements", Journal of Physics: Condensed Matter, vol. 13, No. 4, p. L73-8, Jan. 29, 2001.