Abstract
An austenitic alloy having improved ductility/processability and improved pitting and crevice corrosion resistance comprising, in % by weight, about: 25-30% Ni; 19-23% Cr; 6-8% Mo; 0.3-0.5% N; 0.5% Mn; 0-1.5% Cu; 0-0.2% C; 0-1% Al; 0-0.01% S; 0-1% Ti; 0-1% Si; up to trace amounts of Mg, Ca, and Ce; and balance Fe plus incidental impurities.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A corrosion resistant austenitic alloy consisting essentially of, in % by weight, Ni: 26-30 Cr: 20-22 Mo: 6.5-7.5 N: 0.31-0.35 Mn: 0-5 Cu: 0-1.5 C: 0-0.2 Al: 0-1 S: 0-0.01 Ti: 0-1 Si: 0-1 Mg: up to trace amounts Ca: up to trace amounts Ce: up to trace amounts Fe: balance including incidental impurities; and wherein the alloy has a sigma solvus temperature of less than 2000° F. for improved processability and a pitting resistance equivalent number (PREN) of 50 or greater, wherein: PREN=% Cr+3.3(% Mo)+30% N.
- Claim 2Depends on #1
The alloy of claim 1 , including about 26-29% Ni; 20-22% Cr; 6.5-7.5% Mo and 0.33-0.35% N.
- Claim 3Depends on #1
The alloy of claim 1 , including about 26-28% Ni; 20-21.5% Cr; 6.6-7.5% Mo and 0.33-0.35% N.