Patents
US 6,916,883 B2#18951273 Most CitedExpiredUnited States (USPTO)Utility

Ethylene interpolymer polymerizations

6Forward Citations (#18951273 Global)
0.3/yrCitation Velocity (#26455563 Global)
1.11Citation PageRank (#36275591 Global)
15Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A new process of interpolymerizing ethylene interpolymer products having improved properties, such as increased onset of crystallization temperature, is disclosed. Preferably, the process comprises interpolymerizing a first homogeneous ethylene/alpha-olefin interpolymer and at least one second homogeneous ethylene/alpha-olefin interpolymer using at least two constrained geometry catalysts having different reactivities such that the first ethylene/alpha-olefin interpolymer has a narrow molecular weight distribution (NMWD) with a very high comonomer content and relatively high molecular weight and the second ethylene/alpha-olefin interpolymer has a NMWD with a low comonomer content and a molecular weight lower than that of the first interpolymer. The resultant first homogeneous interpolymer is combined with the resultant second homogeneous interpolymer in appropriate weight ratios resulting in the desired finished polymer structure. The first interpolymer and the second interpolymer can be polymerized in a single reactor or they can be polymerized in separate reactors operated in parallel or series.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An ethylene/alpha-olefin interpolymer product having from about 5 to about 20 weight percent comonomer content, a melt index of from about 0.5 to about 50 grams/10 minutes, an I 10 /I 2 ratio of from about 6 to about 12, and an Mw/Mn of from about 2 to about 6, wherein at least one part of the interpolymer product has a melting point less than about 115° C., while at least another part has a melting point greater than about 120° C.

  2. Claim 2Depends on #1

    The interpolymer product of claim 1 wherein the part of the interpolymer product having a melting point less than about 115° C. is from about 20 to 80 percent of the interpolymer product.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (15)

PatentTitleYearCitations
US 3,491,073 AProcess for the polymerization of olefins197054
US 3,645,992 AProcess for preparation of homogenous random partly crystalline copolymers of ethylene with other alpha-olefins19721,332
US 4,263,422 APolymerization of olefins with dual, independently supported catalysts198128
US 4,530,914 AProcess and catalyst for producing polyethylene having a broad molecular weight distribution1985487
US 4,935,474 AProcess and catalyst for producing polyethylene having a broad molecular weight distribution1990244
US 4,937,299 AProcess and catalyst for producing reactor blend polyolefins1990681
US 4,939,217 AProcess for producing polyolefins and polyolefin catalysts1990253
US 5,026,798 AProcess for producing crystalline poly-α-olefins with a monocyclopentadienyl transition metal catalyst system1991525
US 5,055,438 AOlefin polymerization catalysts1991673
US 5,064,802 AMetal complex compounds19911,083
US 5,082,902 AMethod for reducing cycle time and improving molded part impact energy and ESCR of linear high density polyethylene using a blend of two linear polyethylenes of different densities199253
US 5,189,192 AProcess for preparing addition polymerization catalysts via metal center oxidation1993130
US 5,382,631 ALinear ethylene interpolymer blends of interpolymers having narrow molecular weight and composition distributions1995267
US 6,369,176 B1Process for preparing in a single reactor polymer blends having a broad molecular weight distribution200245
US 6,610,800 B2Process for preparing in a single reactor polymer blends having a broad molecular weight distribution20035

Non-Patent Literature (5)

  • 1991 Polymers, Laminations & Coatings Conference, TAPPJ Proceedings, presented in Feb., 1991. pp. 289-296. A New Family of Linear Ethylene Polymers with Enhanced Sealing Performance , by D. Van der Sanden and R. W. Halle.
  • 1991 Specialty Polyolefins Conference Proceedings. "The Marketing Challenge Created By Single Site Catalysts in Polyolefins" Sep. 24, 1991, (pp. 41-45) by Michael P. Jeffries.
  • Advances in Organometallic Chemistry, pp. 99-148, vol. 18, (1980) "Ziegler-Natta Catalysts" by Hansjorg Sim and Walter Kaminsky.
  • Advances in Polyolefins, by R. B. Seymour and T. Cheng, (1987) "Polymerization of Olefins With A Homogenous Zirconium/Alumoxane Catalyst" pp. 361-371 by W. Kaminsky and H. Hansen.
  • Advances in PolyolefinsBy R. B. Seymour and T. Cheng. (1987) "New Catalysis and Process for Ethylene Polymerization", pp. 337-354, by Karol. B. Wagner. I Levine, G. Goeke, and a A. Noshay.