Patents
US 6,915,664 B2#26189702 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing a fluorine-doped silica powder

4Forward Citations (#26189702 Global)
0.2/yrCitation Velocity (#34843249 Global)
1.23Citation PageRank (#30965151 Global)
20Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a method of doping silica with fluorine. The method described comprises mixing a powder of silica granules with a solid fluorine compound, thermally decomposing the solid fluorine compound under an inert atmosphere, and densifying the granules to obtain dense grains of doped silica. It is preferable to use ammonium bifluoride. The invention is applicable to preparing high index silica glass, in particular for fabricating optical fiber preforms.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a fluorine-doped silica powder for making optical fiber performs, the method comprising the steps of: mixing a solid fluorine compound with silica granules having a specific surface area greater than 30 m 2 /g; thermally decomposing said solid fluorine compound to obtain doped silica granules; and densifying the doped silica granules to obtain doped silica grains.

  2. Claim 2Depends on #1

    A method according to claim 1 , in which the solid fluorine compound is ammonium bifluoride.

  3. Claim 3Depends on #1

    A method according to claim 1 , in which the decomposition temperature of said solid fluorine compound is lower than or equal to 600°/C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 3,535,890 AMethod of making fused silica197034
US 4,043,789 AProcess for manufacturing of phosphoric acid19772
US 4,152,502 ATitanium-modified silyl chromate catalysts for ethylene polymerization19797
US 4,181,623 ACleaning compositions198049
EP 0,281,282 A1Fabrication of high-silica glass article—9
US 5,039,325 AMethod for consolidating doped glass using an encapsulating structure19918
US 5,063,179 AProcess for making non-porous micron-sized high purity silica199166
US 5,064,796 ASupport adjuvant for improved vanadium polymerization catalyst199125
EP 0,629,587 A1Process and apparatus for producing fluoride glass—7
US 5,516,350 AProcess for producing synthetic quartz glass powder199623
US 5,562,752 AProcess of manufacturing vitreous silica product including hydrothermally treating a colloidal sol-gel199615
US 5,888,587 AMethod of manufacturing silica powder and use of such powder in making an optical fiber preform199916
US 6,007,786 ADevice for doping silica powder19998
US 6,047,568 AMethod of manufacturing a silica powder and use of such a powder in making an optical fiber preform200021
US 6,071,487 AMethod of manufacturing a silica powder20008
US 6,071,614 AMicroporous fluorinated silica agglomerate and method of preparing and using same20008
US 6,319,550 B1Method and apparatus for treating silica granules using porous graphite crucible20016
US 6,385,384 B1Glasses containing rare earth fluorides200217
US 6,386,373 B1Process for making silica powder and use of such powder in the manufacture of an optical fiber preform20025
US 2004118155 A1Method of making ultra-dry, Cl-free and F-doped high purity fused silica—34

Non-Patent Literature (2)

  • Material Safety Data Sheet: Ammonium Bifluoride, 5 pages retrieved from online Sep. 15, 2004.
  • Timokhin A R et al: "Chemical Reaction of Ammonium Bifluoride with Quartz Glass" Glass and Ceramis, vol. 42, No. 5-6, May 1985, pp. 267-269.