Plasma curing process for porous low-k materials
Abstract
Low dielectric constant porous materials with improved elastic modulus and hardness. The process of making such porous materials involves providing a porous dielectric material and plasma curing the porous dielectric material to produce a plasma cured porous dielectric material. Plasma curing of the porous dielectric material yields a material with improved modulus and hardness. The improvement in elastic modulus is typically greater than or about 50%, more typically greater than or about 100%, and more typically greater than or about 200%. The improvement in hardness is typically greater than or about 50%. The plasma cured porous dielectric material can optionally be post-plasma treated. The post-plasma treatment of the plasma cured porous dielectric material reduces the dielectric constant of the material while maintaining an improved elastic modulus and hardness as compared to the plasma cured porous dielectric material. The post-plasma treated, plasma cured porous dielectric material has a dielectric constant between about 1.1 and about 3.5 and an improved elastic modulus and hardness.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 5.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for making a plasma cured material from an uncured porous dielectric material comprising: providing the uncured porous dielectric material produced by a spin-on process, the material having a first dielectric constant, having a first elastic modulus, and having a first hardness, wherein the porous dielectric material is selected from a hydrogen silsesquioxane dielectric material or a mixed hydrogen silsesquioxane/methylsilsesquioxane dielectric material, and the porous dielectric material is not a porous methylsilsesquioxane-based dielectric material; exposing the uncured porous diel
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Abstract for JP 59-178749A to Takeda (Fujitsu), Oct. 1984.
- Abstract for JP 63-107122A to Fukuyama et al (Fujitsu), May 1988.
- Glasser et al.; Effect of the H20/TEOS Ratio Upon the Preparation and Nitridation of Silica Sol/Gel Films; Journal of Non-Crystalline SOlids; 1984; 13 pgs.; vol. 63; Elsevier Science Publishers B.V.; North-Holland, Amsterdam, no month.
- Han Q. et al: "Ultra Low-K Porous Silicon Dioxide Films from a Plasma Process", Proceedings of the IEEE, International Interconnect Technology Conference, Jun. 4, 2001, pp. 171-173.
- Kim J-J et al: "The Effects of Plasma Treatment on SiO2 Aerogel Film Using Various Reactive (O<SUB>2</SUB>, H<SUB>2</SUB>, N<SUB>2</SUB>) and Non-Reactive (He, Ar) Gases", Thin Solid Films, Elsevier-Sequoia S.A. Lausanne, CH, vol. 377-378, Dec. 1, 2000, pp. 525-529.