Abstract
A method of growing quaternary epitaxial films having the formula YCZN wherein Y is a Group IV element and Z is a Group III element at temperatures in the range 550-750° C. is provided. In the method, a gaseous flux of precursor H 3 YCN and a vapor flux of Z atoms are introduced into a gas-source molecular beam epitaxial (GSMBE) chamber where they combine to form thin film of YCZN on the substrate. Preferred substrates are silicon, silicon carbide and AlN/silicon structures. Epitaxial thin film SiCAlN and GeCAlN are provided. Bandgap engineering may be achieved by the method by adjusting reaction parameters of the GSMBE process and the relative concentrations of the constituents of the quaternary alloy films. Semiconductor devices produced by the present method have bandgaps from about 2 eV to about 6 eV and exhibit a spectral range from visible to ultraviolet which makes them useful for a variety of optoelectronic and microelectronic applications. Large-area substrates for growth of conventional Group III nitrides and compounds are produced by SiCAlN deposited on large-diameter silicon wafers. The quaternary compounds, especially the boron containing compounds, exhibit extreme har
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 20.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for depositing an epitaxial thin film having the quaternary formula YCZN wherein Y is a Group IV element and Z is a Group III element on a substrate at temperature between ambient temperature and 1000° C. in a gas source molecular beam epitaxial chamber, comprising introducing into said chamber: i. gaseous flux of precursor H 3 YCN wherein H is hydrogen or deuterium; and ii. vapor flux of Z atoms; under conditions whereby said precursor and said Z atoms combine to form epitaxial YCZN on said substrate.
- Claim 2Depends on #1
The method of claim 1 wherein said temperature is about 550° C. to 750° C.
- Claim 3Depends on #1
The method of claim 1 wherein said substrate is silicon or silicon carbide.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 20 total)
References Cited — Backward Prior Art (3)
Non-Patent Literature (5)
- Goldfarb, The Journal of Chemical Physics, "Infrared Spectrum and Structure of Germyl Cyanide", vol. 37, No. 3, pp. 642-646 (1962).
- Jenkins, et al., Journal of Crystal Growth, "Growth of Solid Solutions of Aluminum Nitride and Silicon Carbide by Metalorganic Chemical Vapor Deposition", vol. 128, Nos. 1-4, pp. 375-378 (1993).
- Kern, et al., Journal of Materials Research, Aluminum Nitride-silicon Carbide Solid Solutions Grown by Plasma-assisted, Gas-source Molecular Beam Epitaxy, vol. 13, No. 7, pp. 1816-1822 (1998).
- Kern, et al., Journal of Materials Research, Solid Solutions of AIN and SiC Grown by Plasma-assisted, Gas-source Molecular Beam Epitaxy, vol. 8, No. 7, pp. 1477-1480 (1993).
- MacDiarmid, Journal of Inorganic and Nuclear Chemistry, "Pseudo-halogen Derivatives of Monosilane", vol. 2, No. 2, pp. 88-94 (1956).