Semiconductor device applying to the crystalline semiconductor film
Abstract
There is disclosed a semiconductor device and a method of fabricating the semiconductor device in which a heat treatment time required for crystal growth is shortened and a process is simplified. Two catalytic element introduction regions are arranged at both sides of one active layer and crystallization is made. A boundary portion where crystal growth from one catalytic element introduction region meets crystal growth from the other catalytic element introduction region is formed in a region which becomes a source region or drain region.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An electronic device having an active matrix display device comprising: a thin film transistor having an active layer comprising a crystalline semiconductor film over a substrate having an insulating surface, said active layer comprising at least a channel forming region, a source region, and a drain region, a first wiring electrically connected to the thin film transistor; a leveling film over said thin film transistor the leveling film having an opening to reach the first wiring; a pixel electrode connected to the first wiring through the opening; an alignment film on the pixel electrode; co
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- European Search Report, EPO, Aug. 8, 2000, 4 pages.
- H. Furue et al., "Characteristics and Driving Scheme of Polymer-Stabilized Monostable FLCD Exhibiting Fast Response Time and High Contrast Ratio with Gray-Scale Capability," SID 98 DIGEST, pp. 782-785.
- Ohtani et al., "LP-B: Late-News Poster: A 60-in. HDTV Rear-Projector with Continuous-Grain Silicon Technology," May 17-22, 1998, pp. 467-470, SID 98 Digest, International Symposium Digest of Technical Papers, vol. XXIX.
- R. Shimokawa et al., "Characterization of High-Efficiency Cast-Si Solar Cell Wafers by MBIC Measurement," Japanese Journal of Applied Physics, 1988, vol. 27, No. 5, pp. 751-758.
- S. Inui et al., "Thresholdless antiferroelectricity in liquid crystals and its application to displays," J. Mater. Chem., 1996, 6(4), pp. 671-673.