Storable cementitious slurries containing boric acid and method of using the same
Abstract
A storable, hydraulically-active, cementitious slurry is made and used to cement within subterranean foundations for oil and gas wells. The slurry is made from a hydraulically-active cementitious material, a suspending agent, and, as a retarder, boric acid. The boric acid is present in the cementitious slurry in an amount sufficient to lower the pH of the storable cementitious slurry to at least 12.0, preferably to at least 11.0 or preferably, for reasons of longevity, to a pH of at least 9.0. Generally the amount of boric acid in the cementitious slurry is between from about 1 to about 6 percent by weight. Preferred as suspending agent are iota carrageenan as well as poly (methyl vinyl ether/maleic anhydride) decadiene copolymer. The slurry remains liquid during storage. The slurry is activated when needed for cementing and is pumped into the subterranean formation where it is allowed to set.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 39.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A storable, hydraulically-active, cementitious slurry comprising: a hydraulically-active cementitious material suitable for cementing within subterranean formations for oil or gas wells; a suspending agent; and boric acid wherein the amount of boric acid in the cementitious slurry is between from about 1 to about 6 percent by weight.
- Claim 2Depends on #1
The storable, hydraulically-active, cementitious slurry of claim 1 , wherein the suspending agent is iota carrageenan.
- Claim 3Depends on #1
The storable, hydraulically-active, cementitious slurry of claim 1 , wherein the suspending agent comprises poly (methyl vinyl ether/maleic anhydride) decadiene copolymer.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 39 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (4)
- WPI Abstract Accession No. 1989-003162 & JP 63280189 A (Shimizu Construction Co) 17/11/1988 (see abstract)
- WPI Abstract Accession No. 1996-351301 & JP 08166492 A (Toshiba Ceramics Co) 25/06/1996 (see abstract)
- WPI Abstract No. 1989-003162.
- WPI Abstract No. 1996-351301.