Patents
US 6,906,144 B2#13873162 Most CitedExpiredUnited States (USPTO)Utility

Polypropylene-based resin composition for powder slush molding

8Forward Citations (#13873162 Global)
0.4/yrCitation Velocity (#21164841 Global)
1.52Citation PageRank (#22471730 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A polyproplylene-based resin composition for powder slush molding which is a mixture of a polypropylene homopolymer, copolymer, or terpolymer; an olefin rubber; a styrene rubber; a process oil; and a polypropylene wax, wherein the composition is excellent in low-temperature impact resistance and heat resistance and has no offensive odor. The composition can be formed by a cryofreeze pulverization method in the presence of liquid nitrogen into a powder having an average particle size of 200 to 300 μm suitable for powder slush molding. The powder can be adhered to a polyurethane foamed layer and a surface treating agent without a primer coating. The powder is particularly suitable for forming the interior surface for manufacture of an automobile surface such as an instrument panel.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A polypropylene-based resin composition for powder slush molding comprising: (A) 1 to 40 parts by weight of a polypropylene; (B) 10 to 50 parts by weight of a styrene rubber; (C) 10 to 50 parts by weight of an ethylene-α-olefin copolymer rubber; (D) 1 to 20 parts by weight of a process oil; and (E) 1 to 30 parts by weight of a polypropylene wax with reference to 100 parts by weight of the resin composition.

  2. Claim 2Depends on #1

    The polypropylene-based resin composition for powder slush molding according to claim 1 , wherein said polypropylene is selected from the group consisting of polypropylene homopolymer, propylene-ethylene copolymer, and propylene-ethylene-butene terpolymer and has a melt index of 20 to 70 g/10 min at 230° C. under 2.16 kg of load.

  3. Claim 3Depends on #1

    The polypropylene-based resin composition for powder slush molding according to claim 1 ,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • JP 10-287775, Oct. 27, 1998 (abstract in English only).
  • JP 2000-204207 (English translation).