Patents
US 6,906,134 B2#30037379 Most CitedExpiredUnited States (USPTO)Utility

Thermoplastic resin and preparation thereof

3Forward Citations (#30037379 Global)
0.1/yrCitation Velocity (#39486087 Global)
1.25Citation PageRank (#30182920 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to ABS thermoplastic resin and preparation thereof, and particularly to a process for preparing an ABS graft copolymer comprising the step of introducing to a) 40 to 80 weight parts of rubber latex comprising i) 10 to 50 weight parts of large diameter polybutadiene rubber latex having a particle diameter of 2500 to 3500 Å, gel contents of 60 to 80%, and a swelling index to 12 to 30, and ii) 50 to 90 weight parts of large diameter rubber latex having a particle diameter of 2500 to 3500 Å, gel contents of 81 to 97%, and a swelling index of 18 to 40, b) 20 to 60 weight parts of a monomer mixture of two or more kinds selected from a group consisting of aromatic vinyl compounds and vinyl cyanide compounds to prepare a graft copolymer, wherein 5 to 30 wt % of the monomer mixture is introduced as a batch and simultaneously 70 to 95 wt % of the monomer mixture is started to be continuously introduced in an emulsified state, and a thermoplastic resin composition using the same. According to the process of the present invention, control of polymerization heat is easy even at high solid contents, and polymerization cohesion contents can be minimized and thus ABS

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing an ABS graft copolymer comprising the steps of introducing to a) 40 to 80 weight parts of rubber latex comprising i) 10 to 50 weight parts of large diameter polybutadiene rubber latex having a particle diameter of 2500 to 3500 Å, gel contents of 60 to 80%, and a swelling index to 12 to 30; and ii) 50 to 90 weight parts of large diameter polybutadiene rubber latex having a particle diameter of 2500 to 3500 Å, gel contents of 81 to 97%, and a swelling index of 18 to 40, b) 20 to 60 weight parts of a monomer mixture of two or more kinds selected from a group consisting of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • International Search Report; International application No. PCT/KR02/01884; International filing date Oct. 9, 2002; Jan. 31, 2003.