Abstract

Nylon-intercalated (concentrate nylon), layered silicates, in concentrated form, containing at least 6% to about 40% by weight layered silicate, preferably about 8% to about 30% by weight layered silicate, intercalated with a nylon that is polymerized while in contact with the clay, during ring-opening polymerization of the nylon reactants (monomers) and melt processing. The in-situ nylon polymerization reaction to form the concentrate nylon is continued until the number average molecular weight (Mn) of the nylon is about 25,000 or less, preferably 15,000 or less, more preferably about 5,000-10,000, to maintain melt processability of the resulting concentrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 22.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A nanocomposite concentrate composition consisting of 6% to about 40% by weight of a layered silicate material intercalated with a concentrate polyamide having a number average molecular weight (Mn) of about 25,000 or less and 60% to 94% of a matrix polymer, wherein the polyamide-intercalated layered silicate material is formed by intercalating the layered silicate material with onium ions and a lactam monomer.

  2. Claim 2Depends on #1

    A nanocomposite concentrate composition in accordance with claim 1 , wherein the Mn of the concentrate polyamide is about 15,000 or less.

  3. Claim 3Depends on #2

    A nanocomposite concentrate composition in accordance with claim 2 , wherein the Mn of the concentrate polyamide is in the range of about 5,000 to about 10,000.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Kirk-Othmer, Encyclopedia of Chemical Technology, Fourth Edition, vol. 19, Pigments to Powders, Handling; pp. 471-473 and 485-502 (1996).
  • Usuki et al. J. Mat ResVol. 8, No. 5, May 1993 pp. 1179-1183.