Dielectric filler containing resin for use in formation of built-in capacitor layer of printed wiring board and double-sided copper clad laminate with dielectric layer formed using the same dielectric filler containing resin, and production method of double-sided copper clad laminate
Abstract
An object is to provide a dielectric layer of a double-sided copper clad laminate, for use in formation of a built-in capacitor layer, which can be formed in an optional thickness without using a skeletal material and is provided with a high strength. For the purpose of achieving the object, “a dielectric filler containing resin for use in formation of the built-in capacitor layer of a printed wiring board obtained by mixing a binder resin comprising 20 to 80 parts by weight of epoxy resin (inclusive of a curing agent), 20 to 80 parts by weight of a solvent soluble aromatic polyamide resin polymer, and a curing accelerator added in an appropriate amount according to need; and a dielectric filler which is a nearly spherical dielectric powder having perovskite structure which is 0.1 to 1.0 μm in the average particle size D IA , 0.2 to 2.0 μm in the weight cumulative particle size D 50 based on the laser diffraction scattering particle size distribution measurement method, and 4.5 or less in the coagulation degree represented by D 50 /D IA where the weight cumulative particle size D 50 and the average particle size D IA obtained by the image analysis”; and the like are used.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 15.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A composition for use in the formation of a built-in capacitor layer of a printed wiring board, comprising: a binder resin comprising 20-80 weight % epoxy resin and curing agent and 20-80 weight % of a solvent soluble aromatic polyamide resin polymer; and a dielectric filler comprising a nearly spherical dielectric powder having a perovskite structure which is 0.1 to 1.0 mm in average particle size D IA, 0.2 to 2.0 mm in weight cumulative particle size D 50 based on a laser diffraction scattering particle size distribution measurement method, and a coagulation degree value of 4.5 or less, wh
- Claim 2Depends on #1
The composition according to claim 1 , wherein the aromatic polyamide resin polymer is obtained by reacting an aromatic polyamide with a rubber resin.
- Claim 3Depends on #1
The composition according to claim 1 , w
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗