Patents
US 6,905,558 B2#80215058 Most CitedExpiredUnited States (USPTO)Utility

Billet by continuous casting and manufacturing method for the same

0Forward Citations (#80215058 Global)
0.0/yrCitation Velocity (#80215058 Global)
0.56Citation PageRank (#80215058 Global)
17Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A billet produced by continuous casting having little central segregation, in particular a billet of high carbon steel produced by continuous casting, and a manufacturing method therefor are provided. In the continuous casting billet, the size of the dendritic equiaxed crystal in a billet central portion is reduced to be not more than 6 mm. For this purpose, electromagnetic stirring is performed so that the inclining angle of the primary dendrite within 10 mm of a billet surface layer is increased to be not less than 10°. Furthermore, the mechanical soft reduction is performed during continuous casting so that the diameter of the center porosity in the billet central portion is reduced to be not more than 4 mm. Thereby, in particular in the manufacturing of the continuous casting billet having a carbon content of not less than 0.6% by mass and a billet size of not more than 160 mm can be provided a billet in which breaking troubles in wire drawing after rolling to a rod are reduced by reducing the central segregation in the billet.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A billet produced by continuous casting, containing not less than 0.6% by mass of carbon and comprising dendritic equiaxed crystals of not larger than 6 mm in a central portion of the billet, said dendritic equiaxed crystals being achieved by horizontally stirring molten steel to be continuously cast within a mold of a continuous casting machine, wherein an inclining angle of a primary dendrite within 10 mm of a surface layer in a section perpendicular to a casting direction is not less than 15° relative to a direction perpendicular to that of the surface layer.

  2. Claim 2Depends on #1

    A billet according to claim 1 , wherein the proportion of the dendritic equiaxed crystals at an upper hemisection of the billet is not less than 30%.

  3. Claim 3Depends on #1, #2

    A billet according to claim 1 or 2 , wherein a center porosity in the central portion of the billet has a diameter not larger th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (17)

PatentTitleYearCitations
US 4,030,534 AApparatus for continuous casting using linear magnetic field for core agitation197723
US 4,108,694 AContinuously cast slabs for producing grain-oriented electrical steel sheets having excellent magnetic properties197813
US 4,123,296 AHigh strength steel rod of large gauge197813
GB 2,102,318 AA process for the production of high-strength wire-rod steel suitable for direct drawing—4
US 4,515,203 AContinuous steel casting process19856
US 4,527,615 AElectromagnetic within-mold stirring method of horizontal continuous casting and an apparatus therefor19854
US 4,567,937 AElectromagnetic stirring method and device for double casting type continuous casting apparatus19867
US 4,671,335 AMethod for the continuous production of cast steel strands198711
JP S62192242 AProduction of continuous casting slab for steel plate having excellent internal soundness—10
JP H07100608 AMethod for continuously casting steel—10
JP H07214262 AMethod for preventing center segregation of continuous casting slab—8
WO 9,808,987 A1Process for the production of grain oriented electrical steel strip having high magnetic characteristics, starting from thin slabs—13
JP H10128512 AUnsolidified reduction rolling method for round billet—6
JP H1110299 AMethod for executing rolling-reduction of unsolidified part in cast slab—13
US 5,868,875 ANon-ridging ferritic chromium alloyed steel and method of making199917
US 6,241,004 B1Method and apparatus for continuous casting200119
US 6,296,719 B1Process for the production of grain oriented electrical steel strip having high magnetic characteristics, starting from thin slabs200112