Method of preparation of non-pyrophoric copper-alumina catalysts
Abstract
Provided is a process for preparing a non-pyrophoric catalyst having about 2 to 20 wt. % of a copper component, wherein at least 50 wt. % of the copper component is in the form of a copper oxide, aluminum oxide-spinel. The catalyst can be prepared by forming a mixture of a copper precursor and an alumina precursor, coextruding the mixture, drying the coextrudate and calcining the dried coextrudate at a temperature of at least 600° C. In other aspects, the invention also relates to processes for the activation of copper-based catalysts and for the regeneration of deactivated copper-based catalysts.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 6.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for preparing a non-pyrophoric catalyst, comprising: forming a mixture of a copper precursor and a water-insoluble alumina precursor; coextruding the mixture; drying the coextrudate; and calcining the dried coextrudate at a temperature of at least 600° C. to form the non-pyrophoric catalyst; wherein the non-pyrophoric catalyst comprises about 2 to 20 wt. % of a copper component, and at least 50 wt. % of the copper component is in the form of a copper oxide, aluminum oxide-spinel.
- Claim 2Depends on #1
The process of claim 1 , wherein the non-pyrophoric catalyst comprises at least 80 wt. % of alumina.
- Claim 3Depends on #1
The process of claim 1 , wherein the calcination temperature is at least 650° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (13)
Non-Patent Literature (1)
- Catalyst Handbook 2<SUP>nd </SUP>Ed.; Twigg (ed.) Wolfe Publishing 1989 pp. 315-331.