Method for producing hydro-refining catalyst
Abstract
A method for producing a hydrorefining catalyst has the steps of preparing an impregnation solution containing molybdenum, phosphorus, cobalt and/or nickel, and citric acid, bringing a carrier into contact with the impregnation solution, and then calcinating the carrier in an oxidizing atmosphere at a temperature at which citric acid is removed. In the impregnation solution, a molar ratio of molybdenum/phosphorus is 6 to 13, a molar ratio of (cobalt and nickel)/phosphorus is 0.5 to 7, and a molar ratio of (cobalt and nickel)/citric acid is 0.5 to 2. As for the hydrorefining catalyst obtained by this method, the activity of the catalyst is high, and the catalyst life is long.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing a hydrorefining catalyst containing cobalt and/or nickel, molybdenum, and phosphorus by bringing an impregnation solution into contact with a carrier formed of inorganic porous oxide, the method comprising: preparing, without using any oxidizing agent and reducing agent, the impregnation solution containing cobalt and/or nickel, molybdenum, phosphorus, and citric acid in which a molar ratio of molybdenum/phosphorus is 6 to 13, a molar ratio of (cobalt and nickel)/phosphorus is 0.5 to 7, and a molar ratio of (cobalt and nickel)/citric acid is 0.5 to 2; bringing the carrie
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗