Patents
US 6,902,960 B2#17640163 Most CitedExpiredUnited States (USPTO)Utility

Oxide interface and a method for fabricating oxide thin films

6Forward Citations (#17640163 Global)
0.3/yrCitation Velocity (#26127759 Global)
1.65Citation PageRank (#19740146 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An oxide interface and a method for fabricating an oxide interface are provided. The method comprises forming a silicon layer and an oxide layer overlying the silicon layer. The oxide layer is formed at a temperature of less than 400° C. using an inductively coupled plasma source. In some aspects of the method, the oxide layer is more than 20 nanometers (nm) thick and has a refractive index between 1.45 and 1.47. In some aspects of the method, the oxide layer is formed by plasma oxidizing the silicon layer, producing plasma oxide at a rate of up to approximately 4.4 nm per minute (after one minute). In some aspects of the method, a high-density plasma enhanced chemical vapor deposition (HD-PECVD) process is used to form the oxide layer. In some aspects of the method, the silicon and oxide layers are incorporated into a thin film transistor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating thin film oxides, the method comprising: forming a silicon layer; and, plasma oxidizing the silicon layer to form an oxide layer overlying the silicon layer at a temperature of less than 400° C., using an inductively coupled plasma source.

  2. Claim 2Depends on #1

    The method of claim 1 wherein plasma oxidizing the silicon layer includes: forming the oxide layer more than 20 nanometers (nm) thick; and, forming the oxide layer with a refractive index between approximately 1.45 and 1.47.

  3. Claim 3Depends on #1

    The method of claim 1 wherein plasma oxidizing the silicon layer includes forming oxide at a rate of up to approximately 4.4 nm per minute.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗