Microporous polishing pads

14Forward Citations (#7105100 Global)
0.7/yrCitation Velocity (#11384363 Global)
1.89Citation PageRank (#15901430 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention provides polishing pads for chemical-mechanical polishing comprising a porous foam and a method for their production. In one embodiment, the porous foam has an average pore size of about 50 μm or less, wherein about 75% or more of the pores have a pore size within about 20 μm or less of the average pore size. In another embodiment, porous foam has an average pore size of about 20 μm or less. In yet another embodiment, the porous foam has a multi-modal pore size distribution. The method of production comprises (a) combining a polymer resin with a supercritical gas to produce a single-phase solution and (b) forming a polishing pad from the single-phase solution, wherein the supercritical gas is generated by subjecting a gas to an elevated temperature and pressure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 14.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing a polishing pad substrate comprising: (a) combining a polymer resin with a supercritical gas to produce a single-phase solution, wherein the supercritical gas is generated by subjecting a gas to an elevated temperature and pressure, and (b) forming a polishing pad from the single-phase solution.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the gas does not contain C—H bonds.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the gas comprises nitrogen, carbon dioxide, or combinations thereof.