Patents
US 6,896,834 B2#15488615 Most CitedExpiredUnited States (USPTO)Utility

Method of applying ablative insulation coatings

7Forward Citations (#15488615 Global)
0.3/yrCitation Velocity (#22809072 Global)
1.66Citation PageRank (#19463872 Global)
22Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of forming ablative insulation coatings on aerospace structures and articles produced thereby. The method includes forming a mold having a cavity configured to complementarily receive at least a portion of the structure and directly molding the ablative coating to a surface of the structure by introducing a prepared ablative mixture, such as an epoxy resin, into the mold. The process may desirably include curing at atmospheric pressures to reduce the expense and equipment required in carrying out the process. The method of applying the ablative coating further includes features such as varying the thickness of the ablative coating from one portion of the component to another. Control of the thickness may be effected through use of spacers embedded into the ablative coating and formed of the same or similar material previously cured prior to placement in the mold.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 7.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming an ablative coating on at least a portion of a structure comprisng: forming a mold having a cavity configured to cooperatively receive the at least a portion of the structure; placing the at least a portion of the structure in the cavity of the mold; preforming at least one spacer from a first ablative mixture; placing the at least one spacer between the surface of the structure and a surface of the mold within the mold cavity to establish a desired thickness of the ablative coating; introducing a second ablative mixture that is substantially similar in composition to the f

  2. Claim 2Independent Claim

    The method

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
US 3,177,175 AAblation-resistant resinous compositions19658
US 3,380,941 AAblative thermal insulation composition of a silicone, epoxy resin, cork and curing agent196816
US 3,755,223 AAn epoxy ablative coating containing a silicone resin, a fibrous reinforcing material, and a non-alkali metal phosphate and borate salt mixture197334
US 3,875,106 AAblation compositions and coatings197526
US 4,031,605 AMethod of fabricating combustion chamber liners197710
US 4,041,872 AWrapper, structural shielding device197727
US 4,204,899 ACork-resin ablative insulation for complex surfaces and method for applying the same198023
US 4,546,674 AMethod for providing a tool for forming an article198516
US 4,595,714 AAblative coating composition and product198661
US 4,772,495 ATrowelable ablative coating composition and method of use198822
US 5,064,583 AMethod for applying mold release coating to separator plates for molding printed circuit boards199130
US 5,094,887 AMethod of spraying a mixture of polyol resin, methylene diphenyl diisocyanate, cork flour, and a solvent onto a surface having a primer coat so as to form an ablative coating19926
US 5,212,944 ACarbon and silicone polymer ablative liner material199333
US 5,307,992 AMethod and system for coating a substrate with a reinforced resin matrix199431
US 5,352,312 AMethod of insulating a rocket motor199441
US 5,399,599 AThermoplastic elastomeric internal insulation for rocket motors for low temperature applications199522
US 5,579,998 AMethod for coating a substrate with a reinforced resin matrix199637
US 5,703,178 AHeat ablative coating composition199757
US 5,746,961 AMethod for enhancement of the surfaces of molded plastic products199862
US 5,882,765 AElement made of a reinforced low density heat protective material and method to obtain said element199913
US 5,985,405 AThree dimensionally reinforced ablative/insulative composite199925
US 6,627,697 B2Low density ablator composition200336

Non-Patent Literature (2)

  • Barry, W.T., et al., "A Study of Physical and Chemical Processes Accompanying the Ablation of Castable Charring Epoxy Resins," Chem. Eng. Reviews, No. 48, vol. 60, pp. 99-112.
  • SAE Standard AS5127/1, revision A, paragraph 8.2.*