Abstract

Austenitic alloy for high-temperature strength with improved pourability and manufacturing, of which the composition comprises, in weight-%: 0.010%<carbon<0.04% 0%<nitrogen<0.01% silicon<2% 16%<nickel<19.9% manganese<8% 18.1%<chromium<21% 1.8%<titanium<3% molybdenum<3% copper<3% aluminum<1.5% boron<0.01% vanadium<2% sulfur<0.2% phosphorous<0.04% and possibly up to 0.5% of at least one element chosen from among yttrium, cerium, lanthanum and other rare earths, the remainder being iron and impurities resulting from manufacturing or deoxidizing, the said composition also satisfying the two following relationships: in relationship to the solidification mode: remainder a =eq. Ni a −0.5×eq. Cr a <3.60 where eq. Cr a =Cr+0.7×Si+0.2×Mn+1.37×Mo+3×Ti+6×Al+4×V, and where eq. Ni a =Ni+22×C+0.5×Cu, in relationship to the rate of residual ferrite: remainder b =eq. Ni b −2×eq. Cr b >−41 where eq. Cr b =Cr+0.7×Si+1.37×Mo+3×Ti+6×Al+4×V, and where eq. Ni b =Ni+22×C+0.5×Cu+0.5×Mn.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 7.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    8%<titanium<3% molybdenum<3% copper<3% aluminum<1.5% boron<0.01% vanadium<2% sulfur<0.2% phosphorous<0.04% and up to 0.5% of at least one element selected from the group consisting of yttrium, cerium, lanthanum and other rare earths, the remainder being iron, wherein the alloy satisfies the two following relationships: in relationship to the solidification mode: remainder a =eq. Ni a −0.5×eq. Cr a <3.60 where eq. Cr a =Cr+0.7×Si+0.2×Mn+1.37×Mo+3×Ti+6×Al+4×V, and where eq. Ni a =Ni+22×C+0.5×Cu, in relationship to the rate of residual ferrite: remain

  2. Claim 18Independent Claim

    1%<chromium<21%

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗