The present invention is directed to a process for producing a silicon wafer which, during the heat treatment cycles of essentially any arbitrary electronic device manufacturing process, may form an ideal, non-uniform depth distribution of oxygen precipitates and may additionally contain an axially symmetric region which is substantially free of agglomerated intrinsic point defects. The process including growing a single crystal silicon ingot from molten silicon, and as part of the growth process, controlling (i) a growth velocity, v, (ii) an average axial temperature gradient, G0, during the growth of a constant diameter portion of the crystal over a temperature range from solidification to a temperature of no less than about 1325° C., and (iii) a cooling rate of the crystal from a solidification temperature to about 1,050° C., in order to cause the formation of an axially symmetrical segment which is substantially free of agglomerated intrinsic point defects. A silicon wafer is then sliced from the ingot, subjected to a heat-treatment to form crystal lattice vacancies in the front surface and bulk layers of the wafer and cooled at a rate sufficient to cause a non-uniform vacancy

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 6.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for heat-treating a Cz, single crystal silicon wafer, to influence the precipitation behavior of oxygen in the wafer in a subsequent thermal processing step, the wafer comprising two major, generally parallel surfaces, one of which is a front surface of the wafer and the other of which is a back surface of the wafer, a central plane between the front and back surfaces, a circumferential edge joining the front and back surfaces, a central axis generally perpendicular to the front and back surfaces, a radius extending from the central axis to the circumferential edge, a surface layer w

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,997,368 AElimination of stacking faults in silicon devices: a gettering process197675
US 4,314,595 AMethod of forming nondefective zone in silicon single crystal wafer by two stage-heat treatment1982179
US 4,376,657 AMethod of making fault-free surface zone in semiconductor devices by step-wise heat treating1983107
US 4,437,922 AMethod for tailoring oxygen precipitate particle density and distribution silicon wafers198497
GB 2,137,524 AA process for fabricating a semiconductor material and an apparatus therefor—34
US 4,505,759 AMethod for making a conductive silicon substrate by heat treatment of oxygenated and lightly doped silicon single crystals198570
US 4,548,654 ASurface denuding of silicon wafer1985108
GB 2,182,262 AOxygen containing silicon substrates—44
US 4,851,358 ASemiconductor wafer fabrication with improved control of internal gettering sites using rapid thermal annealing1989142
DE 3,905,626 A1Verfahren und vorrichtung zur zuechtung von siliziumkristallen—45
US 4,868,133 ASemiconductor wafer fabrication with improved control of internal gettering sites using RTA1989107
JP H01242500 AProduction of silicon substrate—21
JP H0232535 AManufacture of silicon substrate for semiconductor device—31
JP H02180789 AProduction of si single crystal—39
JP H02267195 ASilicon single crystal excellent in withstand voltage characteristic of oxide film and production thereof—39
US 4,981,549 AMethod and apparatus for growing silicon crystals199197
JP H039078 ACam plate type piston motor—34
JP H0393700 AHeat treating method and device of silicon single crystal and production device thereof—30
JP H03185831 AManufacture of semiconductor device—16
JP H0442893 ASilicon wafer—15
JP H04108682 ADevice for producing compound semiconductor single crystal and production—33
EP 0,504,837 A2Method and apparatus for producing silicon single crystal—61
JP H04294540 AManufacture of semiconductor device—16
EP 0,536,958 A1Process for producing a semiconductor wafer—78

Non-Patent Literature (5)

  • "Axial Temperature Gradient of Silicon Crystals During Czochralski Growth", Journal of Crystal Growth, vol. 151, pp. 273-277, 1995.
  • Abe, T., "Innovated Silicon Crystal Growth and Wafering Technologies" Electrochemical Society Proceedings, vol. 97, No. 3, pp. 123-133.
  • Abe, T., et al., "Behavior of Point Defects in FZ Silicon Crystals", Semiconductor Silicon 1990, Proceedings of the Sixth International Symposium on Silicon Materials Science and Technology, vol. 90-7, pp. 105-116, 1990.
  • Abe, T., et al., "Defect-Free Surfaces of Bulk Wafers by Combination of RTA and Crystal Growth Conditions".
  • Abe, T., et al., "Dynamic Behavior of Intrinsic Point Defects in FZ and CZ Silicon Crystals," Mat. Res. Soc. Symp. Proc., vol. 262, pp. 3-13, 1992.