US 6,894,751 B2#5404142 Most CitedExpiredUnited States (USPTO)Utility

Process for making an optical compensator film comprising an anisotropic nematic liquid crystal

17Forward Citations (#5404142 Global)
0.8/yrCitation Velocity (#9072714 Global)
2.51Citation PageRank (#10103033 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for making an optical compensator, comprising the steps of coating a orientable resin in a solvent onto a support; drying the resin-containing coating; orienting the resin-containing layer in a predetermined direction; coating a nematic liquid-crystal compound in a solvent carrier onto the orientation layer; drying the nematic liquid-crystal-containing coating; thermally treating the nematic liquid-crystal compound layer, cooling the nematic liquid-crystal compound layer, polymerizing or curing the anisotropic nematic liquid-crystalline layer to form an integral component; and optionally repeating the above steps on top of the integral component so that the optical axis of the first anisotropic nematic liquid-crystal layer is positioned orthogonally relative to the respective optical axis of the second anisotropic nematic liquid-crystal layer about an axis perpendicular to the plane of the support.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 17.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for making an optical compensator, comprising the steps of: a) applying a liquid comprising a nematic liquid-crystal compound in a solvent carrier onto the orientation layer on a transparent support to form a liquid-crystal-containing coating; b) drying the liquid-crystal-containing coating, thereby forming a liquid-crystal-containing layer; c) optionally heating the liquid-crystal-containing layer to a temperature that is above 50° C.; d) cooling the liquid-crystal-containing layer to near or below its isotropic nematic phase transition temperature T c for at least 5 seconds to for