Surface hardened carbon material and process of manufacturing
Abstract
A carbon material is formed by heat-treating a carbonaceous material in a reaction mix of oxides of boron and boron nitride in a nitrogen atmosphere to temperatures of 1600 to 2000° C. The surface of the carbonaceous material is transformed into a carbon material that is resistant to oxidation to temperatures of 900° C., enabling machined components to be utilized for weeks at that temperature. The carbon material is also stable in inert or vacuum environments to temperatures in the range of 1500 to 2000° C., enabling its use as aluminum evaporative boats and the like.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for manufacturing a carbon material that has enhanced oxidation resistance, involving the steps of: embedding a carbonaceous material in a mixture of boron nitride and an oxide of boron wherein the ratio of boron nitride to oxide of boron is sufficient to prevent formation of a glassy mass of boron oxide; and heating the embedded carbonaceous material to a temperature in the range of from about 1600° C. to about 2000° C. at one atmosphere pressure with flowing nitrogen.
- Claim 2Depends on #1
The process of claim 1 wherein said carbonaceous material is selected from graphite, carbon, carbon-carbon composite, glassy carbon, and grafoil.
- Claim 3Depends on #1
The process of claim 1 wherein said oxide of boron comprises at least one boron compound selected from boric acid, borate, boron oxide, borax, and sodium perborate.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (22)
Non-Patent Literature (1)
- English abstract of KR 20902051101 published Jun. 2002.