Transistor fabrication methods comprising selective wet-oxidation

7Forward Citations (#16197604 Global)
0.3/yrCitation Velocity (#23260095 Global)
1.19Citation PageRank (#32770216 Global)
36Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A transistor gate is formed which comprises semiconductive material and conductive metal. Source/drain regions are formed proximate the transistor gate. In one implementation, the transistor gate and source/drain regions are exposed to a gas mixture comprising H 2 O, H 2 , a noble gas and N 2 under conditions effective to oxidize outer surfaces of the source/drain regions. The N 2 is present in the gas mixture at greater than 0% and less than or equal to 20.0% by volume. In one implementation, the transistor gate and source/drain regions are exposed to a gas mixture comprising H 2 O, H 2 , and an inert gas under conditions effective to oxidize outer surfaces of the source/drain regions. The conditions comprise a pressure of greater than room ambient pressure. Other aspects and implementations are contemplated.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 36 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A transistor fabrication method, comprising: forming a transistor gate comprising semiconductive material and conductive metal; forming source/drain regions proximate the transistor gate; and exposing the transistor gate and source/drain regions to a gas mixture comprising H 2 O, H 2 , a noble gas and N 2 under conditions effective to oxidize outer surfaces of the source/drain regions, the N 2 being present in the gas mixture at greater than 0% and less than or equal to 20.0% by volume.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the conductive metal comprises at least one of Ta and Ti.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the N 2 is present in the gas mixture at greater than 0% and less than or equal to 10.0% by volume.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (36)

PatentTitleYearCitations
US 5,040,046 AProcess for forming highly conformal dielectric coatings in the manufacture of integrated circuits and product produced thereby1991171
US 6,093,661 AIntegrated circuitry and semiconductor processing method of forming field effect transistors200041
US 6,114,259 AProcess for treating exposed surfaces of a low dielectric constant carbon doped silicon oxide dielectric material to protect the material from damage2000194
US 6,265,297 B1Ammonia passivation of metal gate electrodes to inhibit oxidation of metal200150
US 6,348,380 B1Use of dilute steam ambient for improvement of flash devices2002234
US 6,358,788 B1Method of fabricating a wordline in a memory array of a semiconductor device200240
US 6,372,657 B1Method for selective etching of oxides200263
US 6,375,194 B1Method for semiconductor wafer processing system200216
US 6,403,497 B1Method of manufacturing semiconductor device by two stage heating of deposited noncrystalline semiconductor200218
US 6,423,617 B1In-situ use of dichloroethene and NH3 in an H2O steam based oxidation system to provide a source of chlorine200211
US 6,440,382 B1Method for producing water for use in manufacturing semiconductors200215
US 6,455,906 B2Gate stack structure with conductive silicide segment that has substantially etched nitride and/or oxynitride defects protruding from its sidewalls200222
US 6,458,714 B1Method of selective oxidation in semiconductor manufacture200250
US 6,468,854 B1Device and method for protecting against oxidation of a conductive layer in said device200212
US 6,472,264 B1Device and method for protecting against oxidation of a conductive layer in said device200216
US 6,471,780 B1Process for fabricating films of uniform properties on semiconductor devices200220
US 6,479,340 B1Device and method for protecting against oxidation of a conductive layer in said device20028
US 6,489,194 B1Device and method for protecting against oxidation of a conductive layer in said device20029
US 6,537,677 B1Process for fabricating films of uniform properties on semiconductor devices200312
US 6,555,487 B1Method of selective oxidation conditions for dielectric conditioning200311
US 6,569,781 B1Method of forming an ultra-thin oxide layer on a silicon substrate by implantation of nitrogen through a sacrificial layer and subsequent annealing prior to oxide formation200317
US 6,576,979 B2Use of selective oxidation conditions for dielectric conditioning200310
US 6,592,777 B2Manufacture and cleaning of a semiconductor200322

Non-Patent Literature (5)

  • Byung Hak Lee, et al. In-situ Barrier Formation for High Reliable W/barrier/poly-Si Gate Using Denudation of WN<SUB>x </SUB>on Polycrystalline Si, IEEE 14.4.1-14.4.4 (1998).
  • Hitoshi Wakabaysahi, et al., An Ultra-Low Resistance and Thermal Stable W/Pn-Poly-Si Gate CMOS Technology Using Si/TiN Buffer Layer, IEEE, pp. 14.6.1-14.6.4 (1998).
  • Koji Kawada, et al. Water Vapor Generator by Catalytic Reactor, pp. 10-16, pre-May 1999.
  • Ohnishi et al., Improving gate oxide integrity (GOI) of a W/WNx/dual-poly Si stacked-gate by using Wet-Hydrogen Oxidation in 0.14-mum CMOS devices, IEEE, 4 pages (1998).
  • Toshiaki Nagahama, et al., Wet Hydrogen Oxidation System for Metal Gate LSI's, pp. 140-143 Pre-May 1999.