Abstract
A method for coating low viscosity materials onto a wafer to form a uniform film. After a wafer is rotated at a first rotation speed, coating solution is dispensed onto the wafer. The wafer is decelerated to a second rotation speed at a first deceleration rate to spread the coating solution. Next, the wafer is slowly decelerated to a third rotation speed at a second deceleration rate considerably lower than the first deceleration rate, so the coating solution reflows to the center of the wafer. The wafer is then quickly accelerated to a fourth rotation speed at a third acceleration rate larger than the first deceleration rate to spread the coating solution again.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 13.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for coating low viscosity materials, comprising: dispensing a coating solution onto a wafer while the wafer is rotated at a first rotation speed; decelerating the wafer to a second rotation speed at a first deceleration rate of 10,000 rpm/sec to spread the coating solution; decelerating the wafer to a third rotation speed at a second deceleration rate of 100 rpm/sec so the coating solution reflows to the center of the wafer; and accelerating the wafer to a fourth rotation speed at a third acceleration rate of 50,000 rpm/sec, thereby spreading the coating solution again.
- Claim 2Depends on #1
The method as claimed in claim 1 , wherein the coating solution is a photoresist solution.
- Claim 3Depends on #1
The method as claimed in claim 1 , wherein the coating solution is an ARC solution.