Process for making lithium titanate
Abstract
A process is provided for making lithium titanate of closely controlled particle size in the range 5 nm to 2000 nm. The process includes re-firing lithium titanate under controlled conditions so that crystallites of the desired particle size are grown. The lithium titanate may be derived from any suitable source. A suitable source of lithium titanate can be from a process that includes evaporation of a blend that contains lithium and titanium to form a mixture containing lithium and titanium compounds that are subsequently calcined to form lithium titanate. The blend of titanium and lithium may be derived from a variety of titanium and lithium precursor materials.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 47 · Forward citations: 51.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for producing lithium titanate comprising: a. preparing a blend comprising titanium and lithium; b. evaporating the blend to form a mixture of lithium titanium compounds, wherein the evaporating is conducted at a temperature above the boiling point of the liquid in the blend but below the temperature where significant reaction of the lithium and the titanium compounds occurs; c. calcining the mixture to form lithium titanate having a particle size between about 5 and 2000 nm and having a surface area between about 27 and 400 m 2 /g.
- Claim 2Depends on #1
The process of claim 1 further comprising crushing the lithium titanate.
- Claim 3Depends on #2
The process of claim 2 further comprising spray drying the lithium titanate.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 51 total)
References Cited — Backward Prior Art (47)
Non-Patent Literature (5)
- Patent Abstracts of Japan, vol. 007, No. 086 (C-161), Apr. 9, 1983 & JP 58 015031 A (Taijirou Okabe), Jan. 28, 1983 abstract.
- Peramunage and Al. D, "Preparation of Micron-Sized Ll<SUB>4</SUB>Tl<SUB>5</SUB>O<SUB>12</SUB>, and its Electrochemistry in Polyacrlonitrile Electrolyte Based Lithium Cells", Journal of the Electrochemical Society, Electrochemical Society, Manchester, New Hampshire, U.S., vol. 145, No. 8, Aug. 1998,
- Peramunage and Al. D, “Preparation of Micron-Sized Ll4Tl5O12, and its Electrochemistry in Polyacrlonitrile Electrolyte Based Lithium Cells”, Journal of the Electrochemical Society, Electrochemical Society, Manchester, New Hampshire, U.S., vol. 145, No. 8, Aug. 1998, pp. 2609-2615.
- Peramunage D. et al., "Preparation and Battery Applications of Micron Sized Ll<SUB>4</SUB>Tl<SUB>5</SUB>O<SUB>12</SUB>," Materials Research Society Symposium Proceedings, Materials Research Society, Pittsburgh, PA., U.S., vol. 498, No. 496, 1998, pp. 359-365.
- Peramunage D. et al., “Preparation and Battery Applications of Micron Sized Ll4Tl5O12,” Materials Research Society Symposium Proceedings, Materials Research Society, Pittsburgh, PA., U.S., vol. 498, No. 496, 1998, pp. 359-365.