Absorbent binder composition and method of making it
Abstract
An absorbent binder composition is provided which is capable of crosslinking after application to a substrate, in the absence of radiation, at a temperature of about 120° C. or less. The absorbent binder composition includes about 15 to about 99.8% by mass monoethylenically unsaturated polymer units, about 0.1 to about 20% by mass polyacrylate ester units having an alkoxysilane functionality, and about 0.1 to about 75% by mass of polymer units selected from polyolefin glycols and polyolefin oxides. The absorbent binder composition can be prepared using a template polymerization process, with the preformed polyolefin glycol or polyolefin oxide serving as a template polymer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 20.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An absorbent binder composition combined with water, the absorbent binder composition comprising a water-soluble ionic polymer capable of sufficient moisture-induced crosslinking within about 10 minutes at a temperature of about 120° C. or less, to reach an absorbent capacity of at least one gram per gram using the centrifuge retention capacity test.
- Claim 2Depends on #1
The absorbent binder composition of claim 1 , comprising about 15 to about 99.8% by mass monoethylenically unsaturated polymer units, about 0.1 to about 20% by mass ester units selected from the group consisting of acrylate and methacrylate ester units that include an alkoxysilane functionality, and about 0.1 to about 75% by mass of units selected from the group consisting of polyolefin glycol and polyolefin oxide units.
- Claim 3Depends on #1
The absorbent binder composition of claim 1 , comprising about 25 to ab
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗