Patents
US 6,881,601 B2#8416331 Most CitedExpiredUnited States (USPTO)Utility

Nitride compound semiconductor, nitride compound semiconductor light emitting device and method of manufacturing the same

12Forward Citations (#8416331 Global)
0.6/yrCitation Velocity (#13837125 Global)
2.31Citation PageRank (#11571691 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A nitride compound semiconductor light-emitting device having a stack of layers including an active layer for a light emitting device and a method of manufacturing the device is disclosed. The method includes the steps of growing a first layer on a substrate at a first temperature to obtain an incomplete crystalline structure including both indium and aluminum and having the composition expressed as In X Al Y Ga 1-X-Y N(0≦X≦1, 0≦Y≦1). The method grows a cap layer on the first layer to cover the first layer, with growth of the cap layer proceeding at a second temperature substantially equal to or below the first temperature. The first layer is heat treated at a third temperature above the first temperature to cause the incomplete crystalline structure to crystallize and to create areas of differing compositions, thus changing the first layer to an active layer. The material of the cap layer is selected to be heat stable during the heat-treating step.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 12.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a nitride compound semiconductor having a stack of layers, the method including: growing a first layer having the composition expressed as InAlN on a substrate at a first temperature, growing a cap layer on the first layer, the cap layer grown at a second temperature substantially equal to or below the first temperature; and heat treating the first layer at a third temperature above the first temperature to form areas in the first layer where the composition is expressed as In X1 Al 1-X1 N(0<X1<1) and other areas in the first layer where the composition is expre

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the heat treating produces a crystal

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • Matsuoka, Takashi; "Unstable Mixing Region in Wurtzite in<SUB>1-x-y </SUB>Ga<SUB>x</SUB>A1<SUB>y</SUB>N"; Proceedings of The Second International Conference on Nitride Semiconductors -ICNS'97-; Oct. 27-31, 1997; pp. 20-21.
  • Mukai, Takashi et al.; "Amber InGaN-Based Light-Emitting Diodes Operable at High Ambient Temperatures"; Jpn. J. Appl. Phys. vol. 37, Part 2, No. 5A; May 1, 1998; pp. L479-481.
  • Nakamura, Shuji et al.; "Superbright Green InGaN Single-Quantum-Well-Structure Light-Emitting Diodes"; Jpn. J. Appl. Phys. vol. 34, Part 2, No. 10B; Oct. 15, 1995; pp. L332-L1335.
  • Yoshimoto, N. et al.; "Photoluminescence of InGaN films growth at high temperature by metalorganic vapor phase epitaxy"; Appl. Phys. Lett. 59 (18): Oct. 28, 1991; pp. 2251-2253.