Abstract

The present invention provides a process for fabricating ultrathin monolayers or ultrathin multilayer films, the process comprising the steps of: introducing positive or negative charge or a material capable of hydrogen-bonding to a substrate and placing the substrate on a spinner(pretreating step); introducing a material (A) bindable with the material deposited on the substrate, and spinning the substrate at 500 rpm to 30000 rpm for 4 to 200 seconds(first coating step); dropping washing solvent onto the substrate after completion of the first coating and spinning the substrate at 500 rpm to 30000 rpm for 4 to 200 sec to remove weakly-bound material (A) and form a thin film (A)(first washing step); introducing another material (B) bindable with the material (A) coated on the substrate and further coating it in the same condition as of the first coating(second coating step), dropping washing solvent onto the substrate after completion of the second coating and spinning the substrate at 500 rpm to 30000 rpm for 4 to 200 sec to remove the weakly-bound material (B) and form a thin film(B)(second washing step), wherein the entire above steps are more than once repeated.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 22.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for fabricating ultrathin multilayer films, the process comprising the steps of: introducing positive or negative charge or a material capable of hydrogen bonding to a substrate and placing said substrate on a spinner to pretreat said substrate; dropping a material (A) bindable with the material deposited onto the substrate, and spinning the substrate 2000 rpm to 6000 rpm for 4 to 200 seconds in a first coating step; dropping washing solvent onto the substrate after completion of the first coating and spinning the substrate at 2000 rpm to 6000 rpm for 4 to 200 sec to remove weakly-bo

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Electroluminescence Studies on Self-Assembled Films of PPV and CdSe Nanoparticles", Gao et al., J. Phys. Chem. B. 1998, 102, 4096-4103.
  • "Mechanism of and Defect Formation in the Self-Assembly of Polymeric Polycation-Montmorillonite Ultrathin Films", Kotov et al., J. Am. Chem. Soc., 1997, 119, 6821-6832.
  • "Metal Nanoparticle/Polymer Superlattice Films: Fabrication and Control of Layer Structure"; Schmitt et al., Adv. Mater., 1997, 9, No. 1, pp. 61-65.
  • "The Pseudo-Ordered Structure in Light Emitting Porous and Nanocrystalline Silicon Films", Wang et al., Appl. Phys. Lett., 70(17), Apr. 28, 1997, 2265-2267.
  • "Tuning the Performance of Layer-by-Layer Assembled Organic Light Emitting Diodes by Controlling the Position of Isolating Clay Barrier.Sheets", Eckle et al., Nano Letters, 2001, vol. 1, No. 1, pp. 45-49.