US 6,875,997 B2#32263660 Most CitedExpiredUnited States (USPTO)Utility

Test patterns and methods of controlling CMP process using the same

3Forward Citations (#32263660 Global)
0.1/yrCitation Velocity (#39640558 Global)
1.11Citation PageRank (#36150373 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A test pattern and a method of controlling a CMP using the same are provided. The test pattern is disposed on a monitoring region of a semiconductor substrate having a main region and a monitoring region. The test pattern includes a planar region and a pattern region. The method comprises setting a correlation between a step difference of a test pattern and an etched thickness of a main pattern, then applying the CMP to a semiconductor substrate having the test pattern and the main pattern for a predetermined time. The step difference of the test pattern is measured and the etched thickness of the main pattern, which corresponds to the step difference of the test pattern, is determined from the correlation. A polishing time is corrected by comparing the determined etched thickness of the main pattern with a reference value, and the corrected polishing time is applied to a subsequent lot or subsequent substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A test pattern for monitoring a chemical mechanical polishing (CMP) process for polishing a semiconductor substrate having a main region and a CMP monitoring region, the test pattern comprising: a planar portion disposed on the CMP monitoring region having a first pattern density; and a patterned portion disposed on the CMP monitoring region having a second pattern density, the patterned portion having the same structure as the main region of the semiconductor substrate, wherein the patterned portion comprises structures with planar top surfaces.

  2. Claim 2Depends on #1

    The test pattern as claimed in claim 1 , wherein the patterned portion has a same pattern density as the main region.

  3. Claim 3Depends on #1

    The test pattern as claimed in claim 1 , wherein the patterned portion and the planar portion have a width of about 10 to 100 μm and a length of about 10 to 100 μm, respec

Technical Overview & Description